Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 158 MPa | 22900 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® 3433R PC 30% GR, provides improved mechanical properties. UV-stabilized. Internal mold release. |
|||
Flexural Yield Strength | 158 - 250 MPa | 22900 - 36300 psi | Average value: 192 MPa Grade Count:14 |
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% an.. |
|||
Flexural Yield Strength | 158 MPa | 22900 psi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP Noryl_HM4025 PPE+PS LNP* Thermocomp* Noryl_HM4025 compound is a 40% Glass/Mineral filled high modulus grade. DTUL 255F (124C). UL94 V-0/V-1/5VA rated in black and gray only (see thicknesses). |
|||
Flexural Yield Strength | 158 MPa | 22900 psi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP Noryl_HM4025 PPE+HIPS (Europe-Africa-Middle East) LNP* Thermocomp* Noryl_HM4025 compound is a 40% Glass/Mineral filled high modulus grade. DTUL 255F (124C). UL94 V-0/V-1/5VA rated in black and gray only (see thicknesses). |