Polymer Property : Flexural Yield Strength = 14.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 14.0 - 27.6 MPa
2030 - 4000 psi
Average value: 19.6 MPa Grade Count:3
Overview of materials for Polytetrafluoroethylene (PTFE), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Molded". Each property range of values reported is minimum and maximum v..
Flexural Yield Strength 14.0 MPa
2030 psi
ASTM D790
Covestro Baydur® 646 Polyurethane Structural Foam RIM, Density 25 pcf, MDI-based 2-Component Liquid System
0.25 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and of..
Flexural Yield Strength 14.0 - 127 MPa
2030 - 18500 psi
Average value: 38.4 MPa Grade Count:143
Overview of materials for Polypropylene, Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced". Each property range of values reported is minimum and maximum values..