Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 128 MPa | 18600 psi | 1.3 mm/min; ASTM D790 |
Ovation Polymers Nemcon™ E ABS 20CF Nemcon E-series products are designed for use in ESDA electronic assembly environments where strict control of ESD and cleanliness are critical. Nemcon E ABS 20CF is a high modulus carbon fiber-rei.. |
|||
Flexural Yield Strength | 128 MPa | 18600 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP COLORCOMP J1000 PES (Europe-Africa-Middle East) LNP* COLORCOMP* J1000 is a compound based on Polyethersulfone resin. |
|||
Flexural Yield Strength | 128 MPa | 18600 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP COLORCOMP J1000R PES (Europe-Africa-Middle East) LNP* COLORCOMP* J1000R is a compound based on Polyethersulfone resin. Added features include : Mold Release |
|||
Flexural Yield Strength | 128 MPa | 18600 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP DFL32P PC LNP* LUBRICOMP* DFL32P is a compound based on Polycarbonate resin containing 10% Glass Fiber, 15% PTFE. Added features include: Internally Lubricated, Exceptional Processing. |
|||
Flexural Yield Strength | 128 MPa | 18600 psi | ASTM D790 |
Solvay Specialty Polymers Amodel® ET-1001 HS Polyphthalamide (PPA) Resin, Dry As Molded
(discontinued **) AMODEL ET-1001 HS resin is an impact modified polyphthalamide (PPA) with exceptional impact strength and practical toughness. AMODEL PPA resins offer high fatigue strength, and good chemical resist.. |
|||
Flexural Yield Strength | 128 MPa | 18600 psi | Bending Strength; ASTM D790 |
EVALCA EVAL® F100 Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 32 mol % Ethylene.Data provided by EVALCA. Applications: Melt phase forming. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produced as a pa.. |
|||
Flexural Yield Strength | 128 MPa | 18600 psi | 50 mm/min; ASTM D790 |
LG Chemical 92HR SAN Resin Heat and chemical resistance, Good mechanical properties, Excellent processability, Superior transparency, Good dimensional stability, Applications include automobile battery cases, water meter case.. |
|||
Flexural Yield Strength | 128 MPa | 18500 psi | ASTM D790 |
Techmer ES HiFill® ABS GM30 LE 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightFeatures: Low ExtractablesInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 128 MPa | 18600 psi | 2.6 mm/min, 100 mm span; ASTM D 790 |
SABIC Innovative Plastics Noryl PKN4717 PPE+PS (Asia Pacific) PPE+PS. Translucent. FDA compliant. High heat. Foam extrusion. Microwavable. Food packaging uses. Solid properties listed.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Yield Strength | 128 MPa | 18600 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp RB008 PA 66 (Europe-Africa-Middle East) LNP* THERMOCOMP* RB008 is a compound based on PA 66 resin containing Glass Bead.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Yield Strength | 128 MPa | 18500 psi | ASTM D790 |
PlastxWorld CEVIAN® B5723 15% GF PBT/ABS Alloy Glass fiber reinforced, heat resistant and flame retarded PBT/ABS alloy.Information provided by PlastxWorld Inc. |
|||
Flexural Yield Strength | 128 MPa | 18500 psi | ASTM D790 |
Clariant Renol PA211G13 Nylon 6, 13% Glass Fiber Data provided by Clariant Masterbatches |
|||
Flexural Yield Strength | 128 MPa | 18500 psi | ASTM D790 |
Clariant Renol PA213G13 Nylon 6, 13% Glass Fiber, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Flexural Yield Strength | 128 MPa | 18500 psi | ASTM D790 |
Clariant Renol PP1100G40 Polypropylene Homopolymer, 40% Glass Fiber, Chemically Coupled Data provided by Clariant Masterbatches |
|||
Flexural Yield Strength | 128 MPa | 18600 psi | 2 mm/min; ISO 178 |
Eurostar Staramide RB008 PA66, 40% Glass Bead Filled, Injection Molded Staramide RB008 is a 40% Glass Bead Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Yield Strength | 128 MPa | 18600 psi | ASTM D790 |
Chem Polymer Chemlon 206 G Nylon 6, 6% Glass Fiber Reinforced A 6% glass fiber reinforced nylon 6 offering improved creep resistance, stiffness, tensile and dimensional stability over unmodified nylon 6 materials.Data provided by the manufacturer, Chem Polymer.. |
|||
Flexural Yield Strength | 128 MPa | 18500 psi | ASTM D790 |
Ravago Manufacturing Americas Hylac® GP30G ABS, 30% Glass Fiber Reinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Flexural Yield Strength | 128 - 207 MPa | 18500 - 30000 psi | Average value: 169 MPa Grade Count:4 |
Overview of materials for Acrylic/Polycarbonate Alloy, Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy, Carbon Fiber Filler". Each property range of values reported is minimum and.. |