Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 114 MPa | 16500 psi | ASTM D790 |
NYCOA 534H PA 6 high viscosity, heat stabilized, nucleated nylon for tubing, sheet, film and moldingInformation provided by NYCOA, Inc. |
|||
Flexural Yield Strength | 114 MPa | 16500 psi | ASTM D790 |
Nylene® NX1440 Nylon 6 Dry as molded. Injection molding grade. Nylene NX1440 is a medium viscosity, fast cycling molding resin. Crystallization initiators provide fast molding cycles through rapid melt set-up. Parts mold.. |
|||
Flexural Yield Strength | 114 MPa | 16500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycolac® INP222 ABS Bulk MMASAN. Provides an economical option for achieving greater melt strength in polymers. |
|||
Flexural Yield Strength | 114 MPa | 16500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® 505RU PC Lexan* 505RU is a glass reinforced,flame retardant(FR)grade with non brominated and non chlorinated FR systems and UV stablization packages. This product is intended for applications to meet WEEE/Ro.. |
|||
Flexural Yield Strength | 114 MPa | 16500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® 505RU PC (Asia Pacific) Lexan* 505RU is a glass reinforced,flame retardant(FR)grade with non brominated and non chlorinated FR systems and UV stablization packages. This product is intended for applications to meet WEEE/Ro.. |
|||
Flexural Yield Strength | 114 MPa | 16500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® 505RU PC (Europe-Africa-Middle East) Lexan* 505RU is a 10% glass reinforced,flame retardant(FR)grade with non brominated and non chlorinated FR systems and UV stablization packages. This product is intended for applications to meet WEE.. |
|||
Flexural Yield Strength | 114 MPa | 16500 psi | ASTM D790 |
Ravago Manufacturing Americas Hylac® GP74G30 ABS, 30% Glass Fiber Reinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Flexural Yield Strength | 114 MPa | 16500 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL PX9406P PPE NORYL* PX9406P resin is an FR (non-halogenated) grade potentially suitable for a variety of electronics applications. RTI (impact) = 105 C. F1 listed in BK color. |
|||
Flexural Yield Strength | 114 MPa | 16500 psi | 6.4 mm; ASTM D790 |
SABIC Innovative Plastics NORYL PX9406P PPE NORYL* PX9406P resin is an FR (non-halogenated) grade potentially suitable for a variety of electronics applications. RTI (impact) = 105 C. F1 listed in BK color. |
|||
Flexural Yield Strength | 114 MPa | 16500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DD0001I PC LNP* STAT-KON* DD0001I is a compound based on Polycarbonate resin containing Carbon Powder. Added features include: ECO FR rating of 94V-0 @ 3.0mm and 94V-1 @ 1.5mm, High Impact. |
|||
Flexural Yield Strength | 114 MPa | 16500 psi | ASTM D790 |
Techmer ES HiFill® PP GF20 CC HF 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized and High FlowInformation provided by .. |
|||
Flexural Yield Strength | 114 MPa | 16500 psi | ASTM D790 |
Techmer ES HiFill® PP GF20 CC LE 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightFeatures: Chemically Coupled and Low ExtractablesInformation provided by TP Composites, .. |
|||
Flexural Yield Strength | 114 MPa | 16500 psi | ASTM D790 |
Techmer ES HiFill® TPX-PBT-01055 60% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral Filler, 60% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 114 MPa | 16500 psi | ASTM D790 |
Techmer ES Plaslube® J-50/10/TF/10 Polycarbonate, 10% GFR, 10% PTFE |
|||
Flexural Yield Strength | 114 MPa | 16500 psi | |
Sumitomo Bakelite Durez® 29502 B Phenolic, Compression Grade Durez 29502 B brown phenolic is a two stage, glass and mineral filled, special purpose molding material with improved mechanical and heat resistant properties. It is formulated for close tolerance .. |
|||
Flexural Yield Strength | 114 MPa | 16500 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL NH6020 PPE+HIPS Noryl NH6020 resin is an unfilled, injection moldable modified polyphenylene ether resin. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 0.8 .. |
|||
Flexural Yield Strength | 114 MPa | 16500 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL NH6020 PPE+HIPS (Asia Pacific) Noryl NH6020 resin is an unfilled, injection moldable modified polyphenylene ether resin. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 0.8 .. |
|||
Flexural Yield Strength | 114 MPa | 16500 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL NH6020 PPE+HIPS (Europe-Africa-Middle East) Noryl* NH6020 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 0.8 mm an.. |
|||
Flexural Yield Strength | 114 MPa | 16500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON AE002 ABS LNP* STAT-KON* AE002 is a compound based on ABS resin containing 10% Carbon Fiber. Added feature of this material is: Electrically Conductive. |
|||
Flexural Yield Strength | 114 MPa | 16500 psi | ASTM D790 |
Cast Nylons Nycast® 6PA-Blue Nylon 6 NYCAST® 6 PA-Blue along with NYCAST® 6 PA-Natural have replaced bronze, brass, steel, and aluminum in various mechanical applications.Data provided by the manufacturer, Cast Nylons Limited.The dat.. |
|||
Flexural Yield Strength | 114 MPa | 16500 psi | ASTM D790 |
Cast Nylons Nycast® 6PA-MoS2 Nylon 6 NYCAST® 6PA-MoS2 is a molybdenum disulphide filled Type 6 cast nylon. Finely divided MoS2 particles are suspended in the melt during polymerization. This gives the NYCAST® 6PA-MoS2 products improv.. |
|||
Flexural Yield Strength | 114 MPa | 16500 psi | ASTM D790 |
Cast Nylons Nycast® 6PA-Natural Nylon 6, Food Grade NYCAST® 6 PA-Natural along with NYCAST® 6 PA-Blue are two of the most widely used cast nylons in industry. Nylons have replaced bronze, brass, steel, and aluminum in various mechanical applicatio.. |
|||
Flexural Yield Strength | 114 MPa | 16500 psi | ASTM D790 |
Chem Polymer Chemlon 100 X Nylon 66, Lubricated GP A medium viscosity, general purpose injection molding grade nylon 66. Internally and externally lubricated for excellent feed and mold release properties.Data provided by the manufacturer, Chem Pol.. |
|||
Flexural Yield Strength | 114 MPa | 16500 psi | ASTM D790 |
Chem Polymer Chemlon 100 Nylon 66, Lubricated GP A medium viscosity, general purpose injection molding grade nylon 66. Internally lubricated for excellent feed and mold release properties.Data provided by the manufacturer, Chem Polymer. |
|||
Flexural Yield Strength | 114 MPa | 16500 psi | ASTM D790 |
Chem Polymer Chemlon 223 Nylon 6, Nucleated A highly nucleated, lubricated nylon 6 intended for applications requiring a faster cycle time. It has increased tensile strength, rigidity, creep resistance and hardness over general purpose nylon.. |