| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Film Tensile Strength at Break, TD | 29.6 MPa | 4290 psi | ASTM D882 |
| Formosa Plastics Formolene® FORMAX® L71709A Film (Hexene Grade) LLDPE
(discontinued **) High Strength Linear Low Density Polyethylene for Film Extrusion Formolene FORMAX® L7 is a high strength linear low density hexene copolymer polyethylene made using a gas-phase process. Film mechan.. |
|||
| Film Tensile Strength at Break, TD | 29.6 MPa | 4290 psi | ASTM D882 |
| Formosa Plastics Formolene® FORMAX® L71709E2 Film (Hexene Grade) LLDPE
(discontinued **) High Strength Linear Low Density Polyethylene for Film Extrusion Formolene FORMAX® L7 is a high strength linear low density hexene copolymer polyethylene made using a gas-phase process. Film mechan.. |
|||
| Film Tensile Strength at Break, TD | 29.6 MPa | 4290 psi | ASTM D882 |
| Formosa Plastics Formolene® FORMAX® L71709H Film (Hexene Grade) LLDPE
(discontinued **) High Strength Linear Low Density Polyethylene for Film Extrusion Formolene FORMAX® L7 is a high strength linear low density hexene copolymer polyethylene made using a gas-phase process. Film mechan.. |
|||
| Film Tensile Strength at Break, TD | 29.6 MPa | 4290 psi | ASTM D882 |
| DuPont™ Surlyn® 1601B Sodium Ionomer Resin for Blown and Cast Film
(discontinued **) Surlyn® 1601B is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, se.. |
|||
| Film Tensile Strength at Break, TD | 29.6 MPa | 4300 psi | ASTM D882 |
| LyondellBasell Petrothene® LP540200 High Density Polyethylene, Film Extrusion Grade PETROTHENE LP540200 is a copolymer resin designed for blown film applications. This resin offers high ESCR, stiffness, excellent appearance and bubble stability. LP540200 is recommended for high str.. |
|||
| Film Tensile Strength at Break, TD | 29.6 MPa | 4290 psi | ASTM-D882 |
| Westlake EB502 12.5% EVA Copolymer Westlake Elevate™ EB502 resin is a fractional melt index 12.5% VA ethylene vinyl acetate copolymer designed for flexible packaging and other films that require excellent toughness and good heat sea.. |
|||
| Film Tensile Strength at Break, TD | 29.6 MPa | 4300 psi | ASTM D882, A 20 in/min |
| Total HDPE HL 535 High Density Polyethylene, Film Resin Polyethylene: Medium molecular weight, high density film resinCharacteristics:High stiffnessGood heat resistanceExcellent bubble stabilityGood compatibility with LDPE and LLDPEApplications:Release .. |
|||
| Film Tensile Strength at Break, TD | 29.6 MPa | 4290 psi | Calculated from mfr's report of 23.3 N/cm per ASTM D828 and the typical thickness |
| DuPont™ Nomex® N196 Paper, 3 mil Nominal Thickness Nomex® Type N196 is a high floc grade of Nomex® paper. This leads to a high degree of saturability combined with high stiffness and mechanical properties. Type N196 is used where good saturabili.. |
|||
| Film Tensile Strength at Break, TD | 29.6 MPa | 4290 psi | ASTM D882 |
| Bapolene® 122F Polyethylene, Film Grade Bapolene LL122F is a general purpose LLDPE for blown film extrusion applications. This resin offers excellent tensile and toughness properties. Contains medium levels of slip/antiblock additives. .. |
|||
| Film Tensile Strength at Break, TD | 29.6 MPa | 4290 psi | ASTM D882 |
| DuPont™ Surlyn® 1601B-2 Sodium Ionomer Resin for Blown and Cast Film
(discontinued **) Surlyn® 1601 B-2 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry,.. |
|||