Polymer Property : Film Tensile Strength at Break, TD = 5900 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 26.5 - 40.7 MPa
3840 - 5900 psi
Average value: 33.8 MPa Grade Count:17
Overview of materials for Ionomer, Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ionomer, Film Grade". Each property range of values reported is minimum and maximum values of appropriat..