Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 48.1 MPa | 6980 psi | ASTM D882 |
ExxonMobil LL 3301.34 Premium High Strength Film Resin
(discontinued **) LL 3001 resins are hexene copolymer LLDPE film resins. Films produced from this resin have excellent tensile, toughness, and drawability properties. LL 3001 resins are available with blown film addi.. |
|||
Film Tensile Strength at Break, TD | 48.1 MPa | 6980 psi | ASTM D882 |
ExxonMobil LL 3301.63 Premium High Strength Film Resin
(discontinued **) LL 3001 resins are hexene copolymer LLDPE film resins. Films produced from this resin have excellent tensile, toughness, and drawability properties. LL 3001 resins are available with blown film addi.. |
|||
Film Tensile Strength at Break, TD | 48.1 MPa | 6980 psi | Ultimate; ASTM D882 |
LG Chemical SEETEC ST308 Linear Low Density Polyethylene, Blown Film Grade Features: Characteristics- Excellent puncture resistance, tear strength. Excellent sealing and optical properties. Comonomer: Octene-1. Additives- Medium slip agent, Medium antiblocking agentApplica.. |
|||
Film Tensile Strength at Break, TD | 48.1 MPa | 6980 psi | Ultimate; ASTM D882 |
LG Chemical SEETEC ST318 Linear Low Density Polyethylene, Blown Film Grade Features: Characteristics- Excellent puncture resistance, tear strength. Excellent sealing and optical properties. Comonomer: Octene-1. Additives- Medium slip agent, Medium antiblocking agentApplica.. |
|||
Film Tensile Strength at Break, TD | 48.1 MPa | 6980 psi | Ultimate; ASTM D882 |
LG Chemical SEETEC SF318 Linear Low Density Polyethylene, Blown Film Grade Features: Characteristics- Good tensile & tear strength, High clarity, mechanical strength & sealing properties. Comonomer: Octene-1. Additives- Medium slip agent, Medium antiblocking agentApplicati.. |
|||
Film Tensile Strength at Break, TD | 48.1 MPa | 6980 psi | Ultimate; ASTM D882 |
LG Chemical SEETEC SN318 Linear Low Density Polyethylene, Blown Film Grade Features: Characteristics- Good tensile & tear strength, High clarity, mechanical strength & sealing properties. Comonomer: Octene-1. Additives- Medium slip agent, Medium antiblocking agentApplicati.. |