Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 42.7 MPa | 6200 psi | ASTM D882 |
Chevron Phillips MarFlex® 7109S LLDPE Blown Film Resin
(discontinued **) Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,.. |
|||
Film Tensile Strength at Break, TD | 42.7 - 72.4 MPa | 6200 - 10500 psi | ASTM D882 |
Honeywell Halar® High Performance E-CTFE Film
(discontinued **) Description: Halar® is a high performance Ethylene-Chlorotrifluoroethylene (E-CTFE) film with excellent mechanical, electrical and release properties. It is non-flammable, and has outstanding chem.. |
|||
Film Tensile Strength at Break, TD | 42.7 MPa | 6200 psi | ASTM D882 |
Chevron Phillips MarFlex® 7109 LLDPE Blown Film Resin Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,.. |
|||
Film Tensile Strength at Break, TD | 42.7 MPa | 6200 psi | ASTM D882 |
ExxonMobil Exceed™ 1018KA Metallocene Polyethylene Resin Product Description: Exceed 1018 resins are metallocene ethylene-hexene copolymer. Films made from Exceed 1018 resin have outstanding tensile, impact strength and puncture. These superior strength p.. |
|||
Film Tensile Strength at Break, TD | 42.7 MPa | 6200 psi | ASTM D882 |
ExxonMobil Exceed™ 1018KA Metallocene Polyethylene Resin (Asia Pacific Grade) Product Description: Exceed 1018 resins are a metallocene ethylene-hexene copolymer. Films made of Exceed 1018 resins have outstanding tensile, impact strength and puncture. These superior propertie.. |
|||
Film Tensile Strength at Break, TD | 42.7 MPa | 6200 psi | ASTM D882 |
ExxonMobil Exceed™ 1018KB Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 1018KB is a metallocene ethylene-hexene copolymers. Films are made of Exceed 1018KB resin have outstanding tensile, impact strength and puncture. These superior strength .. |
|||
Film Tensile Strength at Break, TD | 42.7 MPa | 6200 psi | ASTM D882 |
ExxonMobil Exceed™ 1018LA Metallocene Polyethylene Resin Product Description: Exceed 1018 resins are metallocene ethylene-hexene copolymer. Films made from Exceed 1018 resin have outstanding tensile, impact strength and puncture. These superior strength p.. |
|||
Film Tensile Strength at Break, TD | 42.7 MPa | 6200 psi | ASTM D882 |
ExxonMobil Exceed™ 1018LA Metallocene Polyethylene Resin (Asia Pacific Grade) Product Description: Exceed 1018 resins are a metallocene ethylene-hexene copolymer. Films made of Exceed 1018 resins have outstanding tensile, impact strength and puncture. These superior propertie.. |
|||
Film Tensile Strength at Break, TD | 42.7 MPa | 6200 psi | ASTM D882 |
ExxonMobil Exceed™ 1018MK Metallocene Polyethylene Resin Product Description: Exceed 1018 resins are metallocene ethylene-hexene copolymer. Films made from Exceed 1018 resin have outstanding tensile, impact strength and puncture. These superior strength p.. |
|||
Film Tensile Strength at Break, TD | 42.7 MPa | 6200 psi | ASTM D882 |
Dow DOWLEX™ 2085G Polyethylene Resin DOWLEX™ 2085G is an ethylene-octene copolymer designed for general purpose thin gauge film applications. It is perfect for high strength consumer trash bags/liners. This product can be used in ot.. |
|||
Film Tensile Strength at Break, TD | 42.7 MPa | 6200 psi | ASTM D882 |
ExxonMobil Exceed™ 1018JA Metallocene Polyethylene Resin Product Description: Exceed 1018 resins are metallocene ethylene-hexene copolymer. Films made from Exceed 1018 resin have outstanding tensile, impact strength and puncture. These superior strength p.. |