Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 41.2 MPa | 5980 psi | ASTM D882 |
Chevron Phillips Dynex™ D604D6 Enhanced LLDPE Blown Film Resin
(discontinued **) Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: superior dart impact, optical, hot-tack and heat seal properties, good drawdown, ca.. |
|||
Film Tensile Strength at Break, TD | 41.2 MPa | 5980 psi | ASTM D882 |
ExxonMobil LL 3002.32 Cast Film Resin
(discontinued **) LL 3002.32 is a hexene copolymer LLDPE cast film resin. Films produced from this resin have excellent tensile properties, as well as stiffness and toughness. Combined with good drawdown properties, .. |
|||
Film Tensile Strength at Break, TD | 41.2 MPa | 5980 psi | ASTM D882 |
Chevron Phillips Dynex™ D605C3 Enhanced LLDPE Blown Film Resin
(discontinued **) Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: superior dart impact, optical, hot-tack and heat seal properties, good drawdown, ca.. |