Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 35.2 MPa | 5100 psi | 3 mil; ASTM D882 |
NOVA Chemicals Sclair® FP026-F Octene LLDPE Film Resin Features: Moderate toughness and strengthGood stiffnessEasy processabilityExcellent seal properties Applications: Heavy duty shipping sacks requiring moderate toughness and high stiffnessIndustrial .. |
|||
Film Tensile Strength at Break, TD | 35.2 MPa | 5100 psi | ASTM D882 |
ExxonMobil Escorene® LD 701.ID Blown Film Resin Escorene Ultra LD 701.ID is a fraction melt index, 10.5 wt% vinyl acetate copolymer specialty film resin for applications requiring outstanding heat sealability, strength and toughness, particularly.. |
|||
Film Tensile Strength at Break, TD | 35.2 MPa | 5100 psi | ASTM D882 |
ExxonMobil LL 1001x26 Blown Film Resin Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort.. |
|||
Film Tensile Strength at Break, TD | 35.2 MPa | 5100 psi | ASTM D882 |
ExxonMobil LLDPE LL 1001X26 Linear Low Density Polyethylene Resin Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort.. |
|||
Film Tensile Strength at Break, TD | 35.2 MPa | 5100 psi | ASTM D882 |
ExxonMobil LLDPE LL 1001X31 Linear Low Density Polyethylene Resin Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort.. |
|||
Film Tensile Strength at Break, TD | 35.2 MPa | 5100 psi | ASTM D882 |
ExxonMobil LLDPE LL 1001X72 Linear Low Density Polyethylene Resin Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort.. |
|||
Film Tensile Strength at Break, TD | 35.2 MPa | 5100 psi | ASTM D882 |
ExxonMobil LLDPE LL 1001X74 Linear Low Density Polyethylene Resin Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort.. |
|||
Film Tensile Strength at Break, TD | 35.2 MPa | 5100 psi | ASTM D882 |
ExxonMobil LLDPE LL 1001X76 Linear Low Density Polyethylene Resin Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort.. |
|||
Film Tensile Strength at Break, TD | 35.2 MPa | 5100 psi | ASTM D882 |
ExxonMobil Exceed™ 1018EB Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 1018EB is a metallocene ethylene-hexene copolymers. Films are made of Exceed 1018EB have outstanding tensile, impact, puncture resistance and low temperature properties. .. |