Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 3.32 MPa | 482 psi | |
3M R3127 Repulpable Single-Coated Tapes 3M™ PTFE Glass Cloth Tape R3127 is a single-sided paper tapes coated with a patented, high tack transparent repulpable adhesive on one side and an easy release coating on the backside for smooth u.. |