Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 248 MPa | 36000 psi | 20 in/min, 2.0 in Jaw Separation; ExxonMobil Method |
ExxonMobil Bicor® 70 HSH OPP Film Product Description: Bicor HSH is a one-side treated, one-side sealable, coextruded OPP film designed for use in unsupported plain or surface print high-speed horizontal applications.Availability: .. |
|||
Film Tensile Strength at Break, TD | 248 MPa | 36000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 314 Polyester Film, 200 Gauge Melinex® 314 is a two-side adhesion promoting polyester film with consistently good handling properties.Information provided by DuPont. |
|||
Film Tensile Strength at Break, TD | 248 MPa | 36000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 314 Polyester Film, 92 Gauge Melinex® 314 is a two-side adhesion promoting polyester film with consistently good handling properties.Information provided by DuPont. |
|||
Film Tensile Strength at Break, TD | 248 MPa | 36000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 453 Polyester Film, 142 Gauge Melinex® 453 is an excellent handling, high clarity film with one side pre-treated to promote adhesion to most printing inks and Industrial coatings.Typical Applications: Melinex® 453 is used as a.. |
|||
Film Tensile Strength at Break, TD | 248 MPa | 36000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 453 Polyester Film, 200 Gauge Melinex® 453 is an excellent handling, high clarity film with one side pre-treated to promote adhesion to most printing inks and Industrial coatings.Typical Applications: Melinex® 453 is used as a.. |
|||
Film Tensile Strength at Break, TD | 248 MPa | 36000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 453 Polyester Film, 300 Gauge Melinex® 453 is an excellent handling, high clarity film with one side pre-treated to promote adhesion to most printing inks and Industrial coatings.Typical Applications: Melinex® 453 is used as a.. |
|||
Film Tensile Strength at Break, TD | 248 MPa | 36000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 453 Polyester Film, 400 Gauge Melinex® 453 is an excellent handling, high clarity film with one side pre-treated to promote adhesion to most printing inks and Industrial coatings.Typical Applications: Melinex® 453 is used as a.. |
|||
Film Tensile Strength at Break, TD | 248 MPa | 36000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 453 Polyester Film, 500 Gauge Melinex® 453 is an excellent handling, high clarity film with one side pre-treated to promote adhesion to most printing inks and Industrial coatings.Typical Applications: Melinex® 453 is used as a.. |
|||
Film Tensile Strength at Break, TD | 248 MPa | 36000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 453 Polyester Film, 700 Gauge Melinex® 453 is an excellent handling, high clarity film with one side pre-treated to promote adhesion to most printing inks and Industrial coatings.Typical Applications: Melinex® 453 is used as a.. |
|||
Film Tensile Strength at Break, TD | 248 MPa | 36000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 453 Polyester Film, 92 Gauge Melinex® 453 is an excellent handling, high clarity film with one side pre-treated to promote adhesion to most printing inks and Industrial coatings.Typical Applications: Melinex® 453 is used as a.. |
|||
Film Tensile Strength at Break, TD | 248 MPa | 36000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 454 Polyester Film, 200 Gauge Melinex® 454 is an excellent handling, high clarity film with both sides pre-treated to promote adhesion to most printing inks and Industrial coatings.Typical Applications: Melinex® 454 is used as.. |
|||
Film Tensile Strength at Break, TD | 248 MPa | 36000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 454 Polyester Film, 400 Gauge Melinex® 454 is an excellent handling, high clarity film with both sides pre-treated to promote adhesion to most printing inks and Industrial coatings.Typical Applications: Melinex® 454 is used as.. |
|||
Film Tensile Strength at Break, TD | 248 MPa | 36000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 454 Polyester Film, 500 Gauge Melinex® 454 is an excellent handling, high clarity film with both sides pre-treated to promote adhesion to most printing inks and Industrial coatings.Typical Applications: Melinex® 454 is used as.. |
|||
Film Tensile Strength at Break, TD | 248 MPa | 36000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 454 Polyester Film, 700 Gauge Melinex® 454 is an excellent handling, high clarity film with both sides pre-treated to promote adhesion to most printing inks and Industrial coatings.Typical Applications: Melinex® 454 is used as.. |
|||
Film Tensile Strength at Break, TD | 248 MPa | 36000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 454 Polyester Film, 92 Gauge Melinex® 454 is an excellent handling, high clarity film with both sides pre-treated to promote adhesion to most printing inks and Industrial coatings.Typical Applications: Melinex® 454 is used as.. |
|||
Film Tensile Strength at Break, TD | 248 MPa | 36000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 455 Polyester Film Melinex® 455 is a high clarity polyester film pretreated on one side for slip. It has excellent handling characteristics.General Product Info: Two smooth coatable surfacesLow surface resistivityCan.. |
|||
Film Tensile Strength at Break, TD | 248 MPa | 36000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 456 Polyester Film Melinex® 456 is an excellent handling, high clarity polyester film with both sides pretreated for slip. The two smooth surfaces allow easy top coating.Approvals: UL 94 VTM-2 - for 200 - 700 gauge (.. |
|||
Film Tensile Strength at Break, TD | 248 MPa | 36000 psi | ASTM D882A |
DuPont Teijin Films Melinex® FRP Polyester Film, 92 Gauge Melinex® FRP is designed specifically for embossing and release applications in the fiberglass reinforced panel industry, with consistently good cross-web flatness and handling properties.Informati.. |
|||
Film Tensile Strength at Break, TD | 248 MPa | 36000 psi | ASTM D882 |
DuPont Teijin Films Mylar® LBT-2 Polyester Packaging Film, 92 Gauge Data provided by DuPont Packaging Polymers.Mylar® LBT-2 is an uncoated, transparent, exceptionally strong film used as a substrate for laminating and extrusion coating and as a component of packagi.. |
|||
Film Tensile Strength at Break, TD | 248 MPa | 36000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 6428 Polyester Film, 200 Gauge Melinex® 6428 is a high clarity polyester film. It is pretreated on both film surfaces to promote adhesion to EVA. Melinex® 6428 is a developmental film designed for the photovoltaics industry.Als.. |
|||
Film Tensile Strength at Break, TD | 248 MPa | 36000 psi | ASTM D882 |
DuPont Teijin Films Mylar® M30 Polyester Film, 100 Gauge (25 µm), PVDC Coated
(discontinued **) Data provided by DuPont Packaging Polymers.A transparent polyester packaging film, solvent coated on both sides with a PVDC copolymer. The coating is heat sealable, and is an excellent moisture and.. |
|||
Film Tensile Strength at Break, TD | 248 MPa | 36000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 454 Polyester Film, 142 Gauge Melinex® 454 is an excellent handling, high clarity film with both sides pre-treated to promote adhesion to most printing inks and Industrial coatings.Typical Applications: Melinex® 454 is used as.. |
|||
Film Tensile Strength at Break, TD | 248 MPa | 36000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 454 Polyester Film, 300 Gauge Melinex® 454 is an excellent handling, high clarity film with both sides pre-treated to promote adhesion to most printing inks and Industrial coatings.Typical Applications: Melinex® 454 is used as.. |
|||
Film Tensile Strength at Break, TD | 248 MPa | 36000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 457 Polyester Film, 200 Gauge Melinex® 457 is one side slip, one side adhesion promoting, super clear, polyester film for color proof applications.Also available in 650 gaugeInformation provided by DuPont. |