Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 21.0 MPa | 3050 psi | ISO 527 |
Premix Thermoplastics PRE-ELEC® ESD 4400 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 4400 is a static dissipative thermoplastic compound based on PE-LD. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 4400 has been developed for .. |
|||
Film Tensile Strength at Break, TD | 21.0 MPa | 3050 psi | ASTM D882 |
NOVA Chemicals Sclair® 11L2B Octene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, excellent seal characteristics, easy processability.Applications: Specialty lamination, co-extrusion of food and liquid packaging.Data provided by the manufactur.. |
|||
Film Tensile Strength at Break, TD | 21.0 MPa | 3050 psi | ASTM D882 |
Huntsman Rexell® M3104 Blown Film Extrusion LLDPE
(discontinued **) Linear-low medium density copolymer, cast film extrusion, FDA compliant.Features: Excellent combination of toughness, stiffness, and optics with good temperature resistance.Applications: Diaper film.. |
|||
Film Tensile Strength at Break, TD | 21.0 MPa | 3050 psi | ASTM D882 |
Chevron Phillips 5036 LDPE High Clarity, Impact Film Resin
(discontinued **) Resin Type: Homopolymer; for General Purpose PackagingCharacteristics: Excellent Clarity, Good Impact Strength, High Slip, No Antiblock, Low Coefficient of Friction, Excellent ProcessabilityApplicat.. |
|||
Film Tensile Strength at Break, TD | 21.0 MPa | 3050 psi | ASTM D882 |
Eastman E6838-902F Polyethylene Film
(discontinued **) Polyethylene E6838-902F natural contains slip and antiblock and is suggested for film applicationsApplications/UsesFood - contact applicationsEastman Chemical Company sold its polyethylene business .. |
|||
Film Tensile Strength at Break, TD | 21.0 MPa | 3050 psi | ASTM D882 |
Eastman E6838-899F Polyethylene
(discontinued **) E6838-899F is a low density formulation with no slip or antiblock. It is suggested for film applications requiring high clarity, good tear and impact strength, a wide heat-sealing range, and good pr.. |
|||
Film Tensile Strength at Break, TD | 21.0 MPa | 3050 psi | ASTM D882 |
Eastman E6838-964F Polyethylene
(discontinued **) E6838-964F is a low density formulation with medium slip and medium antiblock. It is suggested for film applications that require a good balance of physical and optical properties.List of Applicati.. |
|||
Film Tensile Strength at Break, TD | 21.0 MPa | 3050 psi | ASTM D882 |
ExxonMobil Escorene® LD-140 LDPE Industrial Film resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A fractional melt index homopolymer resin for production of film with very good toughness.Applications: Heavy duty bags. Data for film properties b.. |
|||
Film Tensile Strength at Break, TD | 21.0 MPa | 3050 psi | ASTM D882 |
Huntsman PE 1008 Film Extrusion Polyethylene
(discontinued **) Homopolymer, and FDA compliant.Features: Superior strength, good machinability, and heat seal characteristics.Applications: Film extrusion: industrial packaging, frozen food, produce bags, shrink, a.. |
|||
Film Tensile Strength at Break, TD | 21.0 MPa | 3050 psi | ASTM D882 |
Huntsman PE1031 Film Extrusion Polyethylene
(discontinued **) Homopolymer, and FDA compliant.Features: Superior strength, good machinability, and heat seal characteristics.Applications: Film extrusion: clarity packaging, frozen food, produce bags, shrink, bund.. |
|||
Film Tensile Strength at Break, TD | 21.0 MPa | 3050 psi | ASTM D882 |
Chevron Phillips HiD® 9606 HDPE Blown Film and Sheet
(discontinued **) Resin Type: ASTM D 4976 Classification: PE 235, A 54502Applications:General Purpose Films and Sheet, Coextruded Film Structures, Deli and Tissue Films, Sheet Thermoforming Applications with Good Str.. |
|||
Film Tensile Strength at Break, TD | 21.0 MPa | 3050 psi | ASTM D882 |
ExxonMobil Escorene® LD-141 EVA Shrink Film Resin, FMI
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A fractional melt index, 2.0% vinyl acetate copolymer film resin with very good toughness and shrink properties. The low melt index gives excellent.. |
|||
Film Tensile Strength at Break, TD | 21.0 MPa | 3050 psi | ASTM D882 |
ExxonMobil Escorene® LD-318 EVA Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 9.0% vinyl acetate copolymer film resin. Film made from LD-318 exhibits superior impact strength and heat sealability.Applications: Primal meat b.. |
|||
Film Tensile Strength at Break, TD | 21.0 MPa | 3050 psi | ASTM D882 |
ExxonMobil Escorene® LD-319 EVA Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 9.0% vinyl acetate copolymer film resin. Film made from LD-319 exhibits superior impact strength and heat sealability.Applications: Primal meat b.. |
|||
Film Tensile Strength at Break, TD | 21.0 MPa | 3050 psi | ASTM D882 |
ExxonMobil Escorene® LD-334 EVA Film Resin, Clarity, High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 4.2% vinyl acetate copolymer, clarity film resin. The low melt index and comonomer context of this resin help produce films with superior impact .. |
|||
Film Tensile Strength at Break, TD | 21.0 MPa | 3050 psi | ASTM D882 |
Petroquimica Triunfo Trithene® TX 8024 LDPE - High Clarity Film The Trithene TX 8024 resin is a low-density polyethylene (LDPE) with high molecular weight and distribution narrow, designed to obtain films with very high clarity and excellent processability. This.. |
|||
Film Tensile Strength at Break, TD | 21.0 MPa | 3050 psi | ASTM D882 |
Metabolix M-veraâ„¢ B5008 Film Grade Compostable Bioplastic B5008 is a compostable film product with 30% biobased carbon content that is ideal for compost bags and can liners used for organic waste diversion and for shopping and retail bags.Features:Meets re.. |
|||
Film Tensile Strength at Break, TD | 21.0 MPa | 3050 psi | ISO R527-1 |
Iran Petrochemical (PCC) 2101TN47 Low Density Polyethylene LDPE 2101TN47 Shrink FilmThis grade enables high speed production of film without blocking.Information provided by Iran Petrochemical Commercial Co. |
|||
Film Tensile Strength at Break, TD | 21.0 MPa | 3050 psi | ASTM-D882 |
Braskem TS7010 LDPE Blown Film Extrusion Polyethylene TS7010 is a low-density polyethylene (LDPE) that presents excellent processability and good mechanical properties. The incorporated additives package warrants a low coefficient of friction (COF) all.. |
|||
Film Tensile Strength at Break, TD | 21.0 MPa | 3050 psi | ASTM-D882 |
Braskem TX7012 LDPE Blown Film Extrusion Polyethylene TX7012 is a low-density polyethylene (LDPE) with medium molecular weight and good processability in traditional extruders with good mechanical properties and productivity, ensuring uniform thickness.. |
|||
Film Tensile Strength at Break, TD | 21.0 MPa | 3050 psi | ASTM D882 |
Huntsman PE1061 Film Extrusion Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Exceptional strength, good machinability and heat seal characteristics.Applications: Film extrusion: high clarity packaging, frozen food, produce bags, shrink.. |
|||
Film Tensile Strength at Break, TD | 21.0 - 48.0 MPa | 3050 - 6960 psi | Average value: 38.8 MPa Grade Count:34 |
Overview of materials for Linear Low Density Polyethylene (LLDPE)/Octene, Film This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE)/Octene, Film". Each property range of values reported is minimum.. |
|||
Film Tensile Strength at Break, TD | 21.0 MPa | 3050 psi | ASTM D882 |
Huntsman PE 1253 EVA Film Extrusion
(discontinued **) 2.5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, good heat seal characteristics.Applications: Film extrusion: general purpose packaging where to.. |
|||
Film Tensile Strength at Break, TD | 21.0 MPa | 3050 psi | ASTM D882 |
NOVA Chemicals Sclair® 11L4B Octene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, excellent seal characteristics.Applications: Specialty lamination, co-extrusion of food and liquid packaging.Data provided by the manufacturer. |
|||
Film Tensile Strength at Break, TD | 21.0 MPa | 3050 psi | ASTM D882 |
Huntsman PE1353 EVA Film Extrusion
(discontinued **) 3.5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: .. |