Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 19.0 MPa | 2760 psi | ISO 527-3 |
Polimeri Europa Riblene® FF 34 Low Density Polyethylene - Blown Film Extrusion Riblene FF 34 is a high molecular weight low density polyethylene (LDPE), with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FF 34 is characterized by a good melt s.. |
|||
Film Tensile Strength at Break, TD | 19.0 MPa | 2760 psi | ASTM D882 |
ExxonMobil LL 1237x98 Cast Film Resin
(discontinued **) LL 1237x70 is a butene LLDPE with improved stiffness. It can be used alone or as a component in packaging and industrial film.Information provided by ExxonMobil Chemical |
|||
Film Tensile Strength at Break, TD | 19.0 MPa | 2760 psi | ASTM D882 |
Eastman E6838-795F Polyethylene
(discontinued **) E6838-795F is a low density formulation with no slip or antiblock level. It is suggested for film applications that require a good balance of properties such as converter film for industrial packag.. |
|||
Film Tensile Strength at Break, TD | 19.0 MPa | 2760 psi | ASTM D882 |
Eastman E6838-796F Polyethylene
(discontinued **) E6838-796F is a low density formulation with no slip or antiblock. It is suggested for film applications requiring a good balance of properties, such as converter film for industrial packaging, gen.. |
|||
Film Tensile Strength at Break, TD | 19.0 MPa | 2760 psi | ASTM D882 |
Eastman E6838-997F Polyethylene
(discontinued **) E6838-997F natural is a low density formulation with no slip or antiblock. Outstanding optical properties make this material an excellent choice for calendering and as a clarity filler in co-extrud.. |
|||
Film Tensile Strength at Break, TD | 19.0 MPa | 2760 psi | ASTM D882 |
Huntsman PE1033 Film Extrusion Polyethylene
(discontinued **) Homopolymer, and FDA compliant.Features: Good opticals, impact strength, good processing properties, and stiffnessApplications: Film extrusion: general purpose packaging and film applications.FDA No.. |
|||
Film Tensile Strength at Break, TD | 19.0 MPa | 2760 psi | ASTM D882 |
ExxonMobil Escorene® LD-144 EVA Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 2% vinyl acetate copolymer packaging film resin. Film made from LD-144 offers improved impact strength and heat sealability compared to homopolym.. |
|||
Film Tensile Strength at Break, TD | 19.0 MPa | 2760 psi | ASTM D882 |
ExxonMobil Escorene® LD-302 EVA Film Resin, High Clarity, High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 3.4% vinyl acetate copolymer, high clarity film resin. The combination of low melt index and comonomer content helps produce films which exhibit .. |
|||
Film Tensile Strength at Break, TD | 19.0 MPa | 2760 psi | ASTM D882 |
ExxonMobil Escorene® LD-303 EVA Film Resin, Clarity, High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 3.8% vinyl acetate copolymer, clarity film resin. The low melt index and comonomer context of this resin help produce films with superior impact .. |
|||
Film Tensile Strength at Break, TD | 19.0 MPa | 2760 psi | ASTM D882 |
ExxonMobil Escorene® LD-307 EVA Film Resin, Clarity, High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 5.0% vinyl acetate copolymer, clarity film resin. Film made from this resin has superior impact strength and heat sealability.Applications: Froze.. |
|||
Film Tensile Strength at Break, TD | 19.0 MPa | 2760 psi | ASTM D882 |
ExxonMobil Escorene® LD-315 EVA Packaging Film Resin for Frozen Food
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 5.0% vinyl acetate copolymer clarity film resin. This resin's low melt index and its comonomer contact combine to provide film of special toughne.. |
|||
Film Tensile Strength at Break, TD | 19.0 MPa | 2760 psi | ASTM D882 |
Huntsman PE1155 EVA Film Extrusion
(discontinued **) 1.5% Vinyl Acetate EVA Copolymer and FDA compliant.Features: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications:.. |
|||
Film Tensile Strength at Break, TD | 19.0 MPa | 2760 psi | ASTM D882 |
Huntsman PE1205 EVA Film Extrusion
(discontinued **) 2% Vinyl Acetate EVA copolymer and FDA compliantFeatures: High clarity film with good stiffness and low temperature toughness.Applications: Film extrusion: food packaging, general purpose packaging .. |
|||
Film Tensile Strength at Break, TD | 19.0 MPa | 2760 psi | ASTM D882 |
Huntsman PE1356 EVA Film Extrusion
(discontinued **) 3.5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: .. |
|||
Film Tensile Strength at Break, TD | 19.0 MPa | 2760 psi | ASTM D882 |
Huntsman PE1407 EVA Film Extrusion
(discontinued **) 4% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: Fi.. |
|||
Film Tensile Strength at Break, TD | 19.0 MPa | 2760 psi | ASTM D882 |
Huntsman PE1507 EVA Film Extrusion
(discontinued **) 5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: Fi.. |
|||
Film Tensile Strength at Break, TD | 19.0 MPa | 2760 psi | ASTM D882 |
Huntsman PE1605 EVA Film Extrusion
(discontinued **) 6% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: Fi.. |
|||
Film Tensile Strength at Break, TD | 19.0 MPa | 2760 psi | ASTM D882 |
Huntsman PE1903 EVA Film Extrusion
(discontinued **) 9% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent toughness and flexibility at low temperatures, and good heat-seal response.Applications: Film extrusion: laminating film, controll.. |
|||
Film Tensile Strength at Break, TD | 19.0 MPa | 2760 psi | ISO 1184 |
Carmel Olefins IPETHENE® 214 Low Density Polyethylene
(discontinued **) IPETHENE® 214 is a general purpose low density polyethylene film extrusion grade. It contains a high level of anti-blocking and slip additives. It is BHT free. APPLICATIONS IPETHENE® 214 is main.. |
|||
Film Tensile Strength at Break, TD | 19.0 MPa | 2760 psi | ASTM D882 |
SCG Chemicals EL-Leneâ„¢ LD1902F Low Density Polyethylene Film Key Characteristics:High strengthGood optical propertiesCan be blended with HDPE, LLDPESafe for food contactContains 1400 ppm slip content and 2400 ppm antiblocking contentRecommended Applications:G.. |
|||
Film Tensile Strength at Break, TD | 19.0 MPa | 2760 psi | ASTM D882 |
SCG Chemicals EL-Leneâ„¢ LD2305F Low Density Polyethylene Film Key Characteristics:Excellent clarity and glossGood zip formationContains 1000 ppm slip agent and 500 ppm antiblocking agentRecommended Applications:Zip bagsGeneral purpose film for food packagingIn.. |
|||
Film Tensile Strength at Break, TD | 19.0 MPa | 2760 psi | |
Dow LDPE 534A Low Density Polyethylene, Blown Film Grade DOW LDPE 534A resin, is a general purpose blown film extrusion resin with excellent drawdown and processability for packaging applications. It contains medium levels of both slip additive and antibl.. |
|||
Film Tensile Strength at Break, TD | 19.0 MPa | 2760 psi | ASTM-D882 |
Braskem LF 118/21 LLDPE Blown Film Extrusion Polyethylene Copolymer LF 118/21 is a LLDPE Butene copolymer produced by Braskem. It was specially designed to provide outstanding processing performance. Films obtained with this grade show good physical and optical prop.. |
|||
Film Tensile Strength at Break, TD | 19.0 MPa | 2760 psi | ISO 1184 |
Carmel Olefins IPETHENE® 213 Low Density Polyethylene IPETHENE® 213 is a general purpose low density polyethylene film extrusion grade. It contains a medium level of anti-blocking and slip additives. It is BHT free. It exhibits a good balance between .. |
|||
Film Tensile Strength at Break, TD | >= 19.0 MPa | >= 2760 psi | ASTM D882 |
Huntsman Rexell® L8102 Cast Film Extrusion LLDPE
(discontinued **) Linear-low density copolymer with high slip and medium antiblock, general purpose blown film extrusion, FDA compliant.Features: Excellent combination of sealability, mechanical strength and optics.A.. |
|||
Film Tensile Strength at Break, TD | >= 19.0 MPa | >= 2760 psi | ASTM D882 |
Huntsman Rexell® L8408 Cast Film Extrusion LLDPE
(discontinued **) Linear-low density copolymer, high quality blown film extrusion, FDA compliant.Features: Excellent combination of sealability, mechanical strength optics, and very low gel levels.Applications: Seali.. |
|||
Film Tensile Strength at Break, TD | 19.0 MPa | 2760 psi | ASTM D882 |
Huntsman PE1345 EVA Film Extrusion
(discontinued **) 3.4% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: .. |
|||
Film Tensile Strength at Break, TD | 19.0 MPa | 2760 psi | ASTM D882 |
Eastman D4036-F Polyethylene
(discontinued **) D4036-F is a low density formulation with high slip and high antiblock. It is suggested for film applications requiring a good balance of properties, such as converter film for industrial and gener.. |