Polymer Property : Film Tensile Strength at Break, TD = 14500 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 100 MPa
14500 psi
ASTM D882
Honeywell Aegisâ„¢ H135MP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H135MP is a lubricated and nucleated high viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR..
Film Tensile Strength at Break, TD 100 MPa
14500 psi
ASTM Data
Styrolution Styrolux 684D SBC
Styrolux 684D is a thermoplastic styrene-butadiene block copolymer which is suitable for injection molding, extrusion, and thermoforming. It offers an outstanding combination of crystal clarity and..
Film Tensile Strength at Break, TD 100 MPa
14500 psi
ISO 527-3
EMS-Grivory Grivory® HB 5299 HV PA*
Product description: Grivory HB 5299 HV is a lubricated, lactam free copolyamide, especially developed for high barrier (oxygen, carbon dioxide) packaging solutions. HV indicates high viscosity, sui..
Film Tensile Strength at Break, TD 100 MPa
14500 psi
ISO 527-3
EMS-Grivory Grivory® HB5299 PA*
Product description: Grivory HB 5299 is a lubricated, lactam free copolyamide, especially developed for high barrier (oxygen, carbon dioxide) packaging solutions. Excellent oxygen and carbon dioxide..