Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 96.5 - 117 MPa | 14000 - 17000 psi | ASTM D882 |
Honeywell Capran® Unidraw (1.00 mil) Nylon 6 Film
(discontinued **) Description: Capran® Unidraw is a 1.00 mil (25 micron) machine direction oriented nylon 6 film specifically designed for the continuous process lamination of glass fiber reinforced panel. High str.. |
|||
Film Tensile Strength at Break, TD | 96.5 MPa | 14000 psi | ASTM D882 |
Honeywell Capran® NyLid™ OMBS-100M Nylon Lidding Film
(discontinued **) Description: Capran® NyLid™ OMBS-100M is a mono-axially oriented, co-extruded Nylon 6/EVOH/Nylong 6 clear film with a print/lamination receptive coating having excellent gas barrier through a broa.. |
|||
Film Tensile Strength at Break, TD | 96.5 MPa | 14000 psi | ASTM D882 |
Dow Saran® 560 Clear Plastic Barrier Film Saran™ 560 is a clear biaxially oriented monolayer barrier film, designed for unit packaging and other applications. It is available in 6 gauge.Information provided by Dow |