Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 21.4 - 39.3 MPa | 3100 - 5700 psi | ASTM D882 |
Honeywell PMP Polymethylpentene Film
(discontinued **) PMP is a clear, red, or blue film manufactured from polymethylpentene. It provides more toughness and heat resistance than standard polyolefins for release film applications.Information provided by.. |
|||
Film Tensile Strength at Break, TD | 26.9 - 39.3 MPa | 3900 - 5700 psi | ASTM D882 |
Honeywell ACLAR® 33C (2.00 mil) Copolymer Film
(discontinued **) Description: ACLAR® 33C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). 33C is used for military and industrial packaging applications.Information provided by Honeywell.. |