Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 221 - 290 MPa | 32000 - 42000 psi | ASTM D882 |
Honeywell Capran® Emblem™ 1000 Bi-Axially Oriented Nylon 6 Film Description: Capran® Emblem™ 1000 is a 0.40 mil (10 micron) biaxially oriented nylon 5 film with excellent flex crack resistance and superior clarity properties. Applications: packaging appl.. |