Polymer Property : Film Tensile Strength at Break, TD = 248 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 179 - 248 MPa
26000 - 36000 psi
Average value: 217 MPa Grade Count:10
Overview of materials for Polyvinyl Dichloride (PVDC) Coated Polyester Film
This property data is a summary of similar materials in the MatWeb database for the category "Polyvinyl Dichloride (PVDC) Coated Polyester Film". Each property range of values reported is minimum an..