Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 90.0 MPa | 13100 psi | ISO 527 |
Victrex® APTIV® 1103-050M Polyetheretherketone (PEEK) Polymer Film, Semi-Crystalline, 30% Mineral Filled Description: APTIV® 1100 series films are the mineral filled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance a.. |
|||
Film Tensile Strength at Break, TD | 90.0 MPa @Thickness 0.100 mm |
13100 psi @Thickness 0.00394 in |
ISO 527 |
Victrex® APTIV® 1103-050M Polyetheretherketone (PEEK) Polymer Film, Semi-Crystalline, 30% Mineral Filled Description: APTIV® 1100 series films are the mineral filled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance a.. |
|||
Film Tensile Strength at Break, TD | 90.0 - 350 MPa | 13100 - 50800 psi | Average value: 180 MPa Grade Count:3 |
Overview of materials for Styrene-Butadiene Copolymer, SBC This property data is a summary of similar materials in the MatWeb database for the category "Styrene-Butadiene Copolymer, SBC". Each property range of values reported is minimum and maximum values .. |
|||
Film Tensile Strength at Break, TD | 90.0 MPa | 13100 psi | ASTM D882 |
Honeywell Aegisâ„¢ H135ZP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H135ZP is a high viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 for nylon.. |
|||
Film Tensile Strength at Break, TD | 90.0 MPa | 13100 psi | ASTM D882 |
Chevron Phillips K-Resin® KR52 Styrene-Butadiene Copolymer Customer Benefits:Excellent Optical PropertiesGood StiffnessExcellent PrintabilityUp to 80% Shrinkage at 100°CBlends well with Polystyrene Typical Applications:Shrink Sleeve LabelsMulti-layer Films.. |
|||
Film Tensile Strength at Break, TD | 90.0 MPa | 13100 psi | ISO 527-3 |
EMS-Grivory Grivory® F 47 H NL nat 6020 PA6 Product description: Grilon F 47 HNL natural 6020 is a nucleated, high viscosity polyamide 6. This product exhibits the following features: Good mechanical propertiesGood barrier against oils and fa.. |
|||
Film Tensile Strength at Break, TD | 90.0 MPa | 13100 psi | ISO 527-3 |
EMS-Grivory Grivory® FG 34 NL nat 6023 PA6 Product description: Grilon FG 34 NL natural 6023 is a modified, medium viscosity polyamide 6. Grilon FG 34 NL natural 6023 exhibits following improvements compared to a PA 6: Better gas barrier pro.. |
|||
Film Tensile Strength at Break, TD | 90.0 MPa | 13100 psi | ISO 527-3 |
EMS-Grivory Grivory® FG 40 NL nat 6018 PA6 Information provided by EMS Grivory |
|||
Film Tensile Strength at Break, TD | 90.0 MPa | 13100 psi | ISO 527-3 |
EMS-Grivory Grivory® FG 40 NL nat 6021 PA6 Product description: Grilon FG 40 NL natural 6021 is a modified, high viscosity polyamide 6. As a result of the modification in comparison to conventional polyamide 6 Grilon FG40 NL natural 6021 off.. |
|||
Film Tensile Strength at Break, TD | 90.0 MPa | 13100 psi | ISO 527-3 |
EMS-Grivory Grivory® FG 40 NL nat 6025 PA6 Product description: Grilon FG 40 NL natural 6025 is a modified, high viscosity polyamide 6. Compared to conventional polyamide 6 Grilon FG40 NL natural 6025 offers the following improvements:Better.. |
|||
Film Tensile Strength at Break, TD | 90.0 MPa | 13100 psi | ISO 527-3 |
EMS-Grivory Grivory® FG 47 NL nat 6028 PA6 Product description: Grilon FG 47 NL natural 6028 is a modified, high viscosity Polyamide 6, which contains also slip and nucleating agents. Grilon FG 47 NL natural 6028 shows following improvements.. |
|||
Film Tensile Strength at Break, TD | 90.0 MPa | 13100 psi | ISO 527-3 |
EMS-Grivory Grivory® F 40 NL PA6 Product description: Grilon F 40 NL natural 6018 is a nucleated and lubricated high viscosity polyamide 6. This product exhibits the following features: Good gas barrierGood mechanical propertiesGoo.. |
|||
Film Tensile Strength at Break, TD | 90.0 MPa | 13100 psi | ISO 527-3 |
EMS-Grivory Grivory® F 47 NL nat 6028 PA6 Product description: Grilon F 47 NL natural 6028 is a nucleated, high viscosity polyamide 6. This product exhibits the following features: Good gas barrierGood mechanical propertiesGood barrier agai.. |
|||
Film Tensile Strength at Break, TD | 90.0 MPa | 13100 psi | ISO 527-3 |
EMS-Grivory Grivory® F 50 nat 6368 PA6 Product description: Grilon F 50 natural 6368 is a modified, very high viscous Polyamide 6 for extrusion processes: Very high melt strengthGood chemical resistanceGood gas-barrierGood mechanical pro.. |