Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 70.0 MPa @Thickness 0.0250 mm |
10200 psi @Thickness 0.000984 in |
ISO 527 |
Victrex® APTIV® 1103-050M Polyetheretherketone (PEEK) Polymer Film, Semi-Crystalline, 30% Mineral Filled Description: APTIV® 1100 series films are the mineral filled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance a.. |
|||
Film Tensile Strength at Break, TD | 70.0 MPa | 10200 psi | ASTM D882 |
DuPont™ Dartek® B-602 Nylon 6,6 Barrier Film, 38 µm Thickness, PVDC Coated
(discontinued **) Data provided by DuPont Packaging Polymers.A strong, transparent nylon 6,6 film which has a PVDC coating applied to one side for enhanced barrier to oxygen, moisture, grease and odor. It is special.. |
|||
Film Tensile Strength at Break, TD | 70.0 MPa | 10200 psi | ASTM D882 |
Honeywell Aegisâ„¢ H155MP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H155MP is a lubricated and nucleated high viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR.. |
|||
Film Tensile Strength at Break, TD | 70.0 MPa | 10200 psi | ASTM D882 |
Solvay Specialty Polymers Ajedium™ Films -- Radel® R-5100 NT15 Polyphenylsulfone (PPSU) Radel® polyphenylsulfone is an amorphous thermoplastic material that offers exceptional hydrolytic stability, and toughness superior to other commercially available, high-temperature films. PPSU .. |
|||
Film Tensile Strength at Break, TD | 70.0 MPa | 10200 psi | ISO 527-3 |
EMS-Grivory Grivory® CR 8 PA* Product description: Grilon CR 8 is a Copolyamide. Grilon CR 8 shows the following features: High flexibility and toughnessGood thermoforming and orientation propertiesHigh shrinkageGood transparen.. |
|||
Film Tensile Strength at Break, TD | 70.0 MPa | 10200 psi | ISO 527-3 |
EMS-Grivory Grivory® L 25 G nat 6011 PA12 Product Description: Grilamid L 25 G natural 6011 is a high viscosity, lubricated polyamide 12. This product has the following features: Very tastelessHigh toughness, even at low temperaturesGood re.. |
|||
Film Tensile Strength at Break, TD | 70.0 MPa | 10200 psi | ISO 527-3 |
EMS-Grivory Grivory® L 25 nat PA12 Product Description: Grilamid L 25 is a high viscosity polyamide 12. This product has the following features: Very tasteless High toughness, even at low temperatures Good resistance to weathering Go.. |