Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 64.5 MPa | 9360 psi | ASTM D822 |
LyondellBasell Alathon® L5906 High Density Polyethylene ApplicationsALATHON XL 5906 is a high molecular weight high density polyethylene homopolymer with a broad bimodal molecular weight distribution. This resin exhibits excellent stiffness, very high t.. |
|||
Film Tensile Strength at Break, TD | >= 64.5 MPa | >= 9350 psi | 200 N/10mm |
Dr. D. Mueller Flexiso® DMD FI 14010 00310 Polyester Electrical Insulation Structure: Flexiso® DMD, FI 14010 00310 is a flexible three layer material, consisting of a layer of polyester film, of which both sides have a layer of polyester fleece fabric and is coated with .. |