Polymer Property : Film Tensile Strength at Break, TD = 6.11 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 6.11 MPa
886 psi
ASTM D3759
3M Scotch® 605 Transparent Film Tape
Scotch® Transparent Film Tape 605 is designed for various light-duty packaging applications such as attaching, mending, gift wrapping, holding and L-Clips. This product offers good performance over..