Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 39.91 MPa | 5788 psi | ASTM D882 |
Dow DOWLEX™ 2036G Linear Low Density Polyethylene Improved thermal stability for high stiffness film applications Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow |