Polymer Property : Film Tensile Strength at Break, TD = 29.7 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 29.7 MPa
4310 psi
Dow Elite® 5200 Linear Low Density Polyethylene