Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 24.1 MPa | 3500 psi | D638 |
Westlake EF528 18.5% Ethylene Vinyl Acetate Copolymer Westlake ELEVATE™ EF528 is an ethylene vinyl acetate copolymer with 18.5% VA. EF528 is designed for blown and cast films requiring excellent optics and low heat seal initiation. High melt strength .. |
|||
Film Tensile Strength at Break, TD | 24.1 MPa | 3500 psi | ASTM D638 |
Westlake Elevate™ DA528AA 18.5% Ethylene Vinyl Acetate Copolymer Westlake ELEVATE™ DA528 is an ethylene vinyl acetate copolymer with 18.5% VA. DA528 is designed for blown and
cast films requiring excellent optics and low heat seal initiation. High melt strength.. |
|||
Film Tensile Strength at Break, TD | 24.1 MPa | 3500 psi | ASTM D882 |
Westlake Elevate™ DA528AA Ethylene Vinyl Acetate Copolymer Developmental ProductDescription: Westlake ELEVATE™ DA528 is an ethylene vinyl acetate copolymer with 18.5% VA. DA528 is designed for blown and cast films requiring excellent optics and low heat s.. |
|||
Film Tensile Strength at Break, TD | 24.1 MPa | 3500 psi | D638 |
Westlake ELEVATE™ EF529 18.5% Ethylene Vinyl Acetate Copolymer Westlake ELEVATE™ EF529 is an ethylene vinyl acetate copolymer with 18.5% VA. It contains no slip or antiblock and is designed for blown and cast films requiring excellent optics and low heat seal .. |
|||
Film Tensile Strength at Break, TD | 24.1 MPa | 3500 psi | ASTM D882 |
ExxonMobil Escorene™ FL 00309 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: FL 00309 is a copolymer of ethylene and vinyl acetate. Processing Conditions: Processing temperatures above 270°C (513°F) may cause resin degradation. Availability: Africa & M.. |
|||
Film Tensile Strength at Break, TD | 24.1 MPa | 3500 psi | Calculated from mfr's report of 19 N/cm per ASTM D828 and the typical thickness |
DuPont™ Nomex® 418 Paper, 3 mil Nominal Thickness Nomex® Type 418 is designed for high-voltage applications such as motor conductor and coil wrap, transformer ground and layer insulation. It can be readily impregnated with varnishes. This calen.. |
|||
Film Tensile Strength at Break, TD | 24.1 MPa | 3500 psi | ASTM D882 |
ExxonMobil LD 051.LQ Shrink Film Resin L Product Description: LD 051.LQ blown film resin is a fractional melt index grade designed for demanding heavy duty film applications, and combines excellent strength properties with outstanding pr.. |
|||
Film Tensile Strength at Break, TD | 24.1 MPa | 3500 psi | ASTM D882 |
ExxonMobil LD 103.59 Industrial Film Resin Product Description: LD 103 resins are homopolymer industrial film resins with excellent toughness. LD 103 resins have a low melt index, which provides good impact strength and melt strength over a .. |
|||
Film Tensile Strength at Break, TD | 24.1 MPa | 3500 psi | ASTM D882 |
ExxonMobil LDPE LD 051.LQ Low Density Polyethylene Resin Product Description: LD 051.LQ blown film resin is a fractional melt index grade designed for demanding heavy duty film applications, and combines excellent strength properties with outstanding proc.. |
|||
Film Tensile Strength at Break, TD | 24.1 MPa | 3500 psi | ASTM D882 |
ExxonMobil LDPE LD 103.09 Low Density Polyethylene Resin Product Description: LD 103 resins are homopolymer industrial film resins with excellent toughness. LD 103 resins have a low melt index, which provides good impact strength and melt strength over a .. |
|||
Film Tensile Strength at Break, TD | 24.1 MPa | 3500 psi | ASTM D882 |
ExxonMobil LDPE LD 103.59 Low Density Polyethylene Resin Product Description: LD 103 resins are homopolymer industrial film resins with excellent toughness. LD 103 resins have a low melt index, which provides good impact strength and melt strength over a .. |
|||
Film Tensile Strength at Break, TD | 24.1 MPa | 3500 psi | ASTM D882 |
ExxonMobil LDPE LD 123.LN Low Density Polyethylene Resin Product Description: LD 123.LN blown film grade offers an excellent balance of optical and strength properties for general purpose clear film applications.Availability: Latin America, North America .. |
|||
Film Tensile Strength at Break, TD | 24.1 MPa | 3500 psi | ASTM D882 |
ExxonMobil LDPE LD 157CW Blown Low Density Polyethylene Resin Product Description: LD 157CW offer good mechanical properties as well as excellent opticals.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: NoThermal Stabilizer: YesAppl.. |
|||
Film Tensile Strength at Break, TD | 24.1 MPa | 3500 psi | ASTM D882 |
ExxonMobil LDPE LD 306.57 Low Density Polyethylene Resin Product Description: LD 306 resins are 5.5% vinyl acetate copolymer, high clarity film resins. Film made from these resins exhibit superior impact strength and heat sealability.Availability: Latin A.. |
|||
Film Tensile Strength at Break, TD | 24.1 MPa | 3500 psi | ASTM D882 |
ExxonMobil LDPE LD 306.75 Low Density Polyethylene Resin Product Description: LD 306 resins are 5.5% vinyl acetate copolymer, high clarity film resins. Film made from these resins exhibit superior impact strength and heat sealability.Availability: Latin A.. |
|||
Film Tensile Strength at Break, TD | 24.1 MPa | 3500 psi | ASTM D882 |
ExxonMobil LDPE LD 363BR Low Density Polyethylene Resin Product Description: LD 363 series are LEVA LDPE grades, offering good optical and mechanical properties. Two additive combinations are available according to the required surface properties.Availab.. |
|||
Film Tensile Strength at Break, TD | 24.1 MPa | 3500 psi | ASTM D882 |
ExxonMobil LDPE LD 363BW Low Density Polyethylene Resin Product Description: LD 363 series are LEVA LDPE grades, offering good optical and mechanical properties. Two additive combinations are available according to the required surface properties.Availab.. |
|||
Film Tensile Strength at Break, TD | 24.1 MPa | 3500 psi | ASTM D882 |
ExxonMobil LDPE LD 380BA Blown Low Density Polyethylene Resin (European Grade) Product Description: LD 380BA offers good toughness and optical properties.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: NoApplications: Coextrus.. |
|||
Film Tensile Strength at Break, TD | 24.1 MPa | 3500 psi | ASTM D882 |
ExxonMobil LLDPE LL 1004YB Film Linear Low Density Polyethylene Resin (European Grade) Product Description: LL 1004YB is an LLDPE grade, offering excellent high temperature stability. Properties may be further enhanced by the combination with Exceed mLLDPE. Availability: Africa & Midd.. |
|||
Film Tensile Strength at Break, TD | 24.1 MPa | 3500 psi | ASTM D882 |
ExxonMobil LLDPE LL 1236.85 Linear Low Density Polyethylene Resin Product Description: LL 1236 Series resins are butane LLDPEs with increased stiffness and a high melt index. They can be used alone or as a component in packaging and industrial film, blown or cast... |
|||
Film Tensile Strength at Break, TD | 24.1 MPa | 3500 psi | ASTM D882 |
ExxonMobil LLDPE LL 1236.86 Linear Low Density Polyethylene Resin Product Description: LL 1236 Series resins are butane LLDPEs with increased stiffness and a high melt index. They can be used alone or as a component in packaging and industrial film, blown or cast... |
|||
Film Tensile Strength at Break, TD | 24.1 MPa | 3490 psi | ASTM D882 |
Dow 662I Low Density Polyethylene Resin Blown Film Resin designed for enhanced bubble stability High melt strength Optimum gauge range: 1.5 - 5.0 mil Complies with U.S. FDA 21 CFR 177.1520 (c) 2.1 Information provided by Dow |
|||
Film Tensile Strength at Break, TD | 24.1 MPa | 3500 psi | ASTM D882 |
ExxonMobil LDPE LD 306.38 Low Density Polyethylene Resin Product Description: LD 306 resins are 5.5% vinyl acetate copolymer, high clarity film resins. Film made from these resins exhibit superior impact strength and heat sealability.Availability: Latin A.. |
|||
Film Tensile Strength at Break, TD | 24.1 MPa | 3500 psi | ASTM D882 |
Amco PRIMATOP LLDPE 009919B Linear Low Density Polyethylene, Butene Copolymer for Film LLDPE 009919B features excellent toughness and strength when drawn down to thin gauges. Applications include blending resin, industrial packaging, coextrusion, industrial liners, and garment bags.Fo.. |