Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 235 MPa | 34100 psi | ASTM D882A |
DuPont Teijin Films Mylar® 800C Polyester Packaging Film, 75 Gauge Data provided by DuPont Packaging Polymers.Melinex® 800C is a clear, one side corona treated polyester film suitable for flexible packaging, printing and laminations. Melinex® 800C is a polyester.. |
|||
Film Tensile Strength at Break, TD | 235 MPa | 34100 psi | ASTM D882A |
DuPont Teijin Films Mylar® 800C Polyester Packaging Film, 48 Gauge Data provided by DuPont Packaging Polymers.Melinex® 800C is a clear, one side corona treated polyester film suitable for flexible packaging, printing and laminations. Melinex® 800C is a polyester.. |