Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 23.2 MPa | 3370 psi | ASTM D882 |
ExxonMobil LD 302.20 High Clarity, High Impact Film Resin LD 302 Series films exhibit superior impact strength, good heat sealability, and good low temperature properties. Typical applications are frozen food packaging or other food packaging.Information .. |
|||
Film Tensile Strength at Break, TD | 23.2 MPa | 3370 psi | ASTM D882 |
ExxonMobil LD 302.32 High Clarity, High Impact Film Resin LD 302 Series films exhibit superior impact strength, good heat sealability, and good low temperature properties. Typical applications are frozen food packaging or other food packaging.Information .. |
|||
Film Tensile Strength at Break, TD | 23.2 MPa | 3370 psi | ASTM D882 |
ExxonMobil LD 302.34 High Clarity, High Impact Film Resin LD 302 Series films exhibit superior impact strength, good heat sealability, and good low temperature properties. Typical applications are frozen food packaging or other food packaging.Information .. |
|||
Film Tensile Strength at Break, TD | 23.2 MPa | 3370 psi | ASTM D882 |
ExxonMobil LD 302.56 High Clarity, High Impact Film Resin LD 302 Series films exhibit superior impact strength, good heat sealability, and good low temperature properties. Typical applications are frozen food packaging or other food packaging.Information .. |
|||
Film Tensile Strength at Break, TD | 23.2 MPa | 3360 psi | ASTM D882 |
ExxonMobil LD 334.57 Clear, High Impact Film Resin LD 334 resins produce films with superior impact strength, good heat sealability, and low temperature properties.Information provided by ExxonMobil Chemical |
|||
Film Tensile Strength at Break, TD | 23.2 MPa | 3360 psi | ASTM D882 |
ExxonMobil LD 334.82 Clear, High Impact Film Resin LD 334 resins produce films with superior impact strength, good heat sealability, and low temperature properties.Information provided by ExxonMobil Chemical |