Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 19.7 MPa | 2860 psi | ASTM D882 |
Westlake EMAC® SP2255 17% Ethylene-Methyl Acrylate Copolymer Westlake EMAC® SP2255 is a 17% EMA copolymer containing slip and antiblock. This resin is designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low heat s.. |