Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 165 MPa | 24000 psi | 20 in/min, 2.0 in Jaw Separation; ExxonMobil Method |
ExxonMobil Label-Lyte™ 70LS447 OPP Film Product Description: A two-side coated, shrink resistant, white, polypropylene film designed for use in hot melt cut-and stack labeling. It has an static resistant, matte finish, paper like print su.. |
|||
Film Tensile Strength at Break, TD | 165 MPa | 24000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 342 Polyester Film Melinex® 342 is a two-side heat-sealable, clear polyester film which is ideal in specialty card laminate applications. This film can be heat sealed to itself and other polyesters, as well as a vari.. |
|||
Film Tensile Strength at Break, TD | 165 MPa | 24000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 547 Polyester Film, 400 Gauge Information provided by DuPont. |
|||
Film Tensile Strength at Break, TD | 165 MPa | 24000 psi | ASTM D882A |
DuPont Teijin Films Melinex® AG2 Polyester Film Melinex® AG2 is a clear polyester film coated on both sides for Anti-fog and Anti-glare performanceTypical Applications: Typical applications include disposable face shields, visors, and other temp.. |
|||
Film Tensile Strength at Break, TD | 165 MPa | 24000 psi | ASTM D882A |
DuPont Teijin Films Melinex® ST328 Polyester Film, 1400 Gauge Melinex® ST328 is an exceptionally white, opaque film with a satin finish. It is pretreated on both surfaces to promote adhesion to a wide range of solvent-based and UV-curable graphics inks and va.. |
|||
Film Tensile Strength at Break, TD | 165 MPa | 24000 psi | ASTM D882A |
DuPont Teijin Films Melinex® ST329 Polyester Film, 1000 Gauge MELINEX® ST329 has good handling properties and a unique pearlescent appearance with no pre-treatments. It is heat stabilized for applications in high temperature processes where film registration .. |
|||
Film Tensile Strength at Break, TD | 165 MPa | 24000 psi | ASTM D882A |
DuPont Teijin Films Mylar® E Polyester Film, 48 Gauge Mylar® E polyester film is a clear smooth base film engineered to provide superior optical and physical properties required of critical dying, metallizing, laminating, labeling and coating applicat.. |
|||
Film Tensile Strength at Break, TD | 165 MPa | 24000 psi | ASTM D882A |
DuPont Teijin Films Mylar® EC Polyester Film, 500 Gauge Mylar® EC films are electrical grade films designed for use in applications where improved dimensional stability is required. In addition to lower levels of shrinkage, Mylar® EC films offer outsta.. |
|||
Film Tensile Strength at Break, TD | 165 MPa | 24000 psi | ASTM D882A |
DuPont Teijin Films Melinex® AF Polyester Film Melinex® AF is a clear polyester film coated both sides with an anti-fog coating. Typical Applications: Typical applications include face shields, masks, visors, and other industrial uses.Informati.. |