Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 159 MPa | 23000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 329 Polyester Film, 1000 Gauge Melinex® 329 is an opaque white, non-pretreated, polyester film with good handling properties and a unique glossy appearance. It is used as a base for pressure sensitive labels, in security and ac.. |
|||
Film Tensile Strength at Break, TD | 159 MPa | 23000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 329 Polyester Film, 1400 Gauge Melinex® 329 is an opaque white, non-pretreated, polyester film with good handling properties and a unique glossy appearance. It is used as a base for pressure sensitive labels, in security and ac.. |
|||
Film Tensile Strength at Break, TD | 159 MPa | 23000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 329 Polyester Film, 142 Gauge Melinex® 329 is an opaque white, non-pretreated, polyester film with good handling properties and a unique glossy appearance. It is used as a base for pressure sensitive labels, in security and ac.. |
|||
Film Tensile Strength at Break, TD | 159 MPa | 23000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 329 Polyester Film, 200 Gauge Melinex® 329 is an opaque white, non-pretreated, polyester film with good handling properties and a unique glossy appearance. It is used as a base for pressure sensitive labels, in security and ac.. |
|||
Film Tensile Strength at Break, TD | 159 MPa | 23000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 329 Polyester Film, 300 Gauge Melinex® 329 is an opaque white, non-pretreated, polyester film with good handling properties and a unique glossy appearance. It is used as a base for pressure sensitive labels, in security and ac.. |
|||
Film Tensile Strength at Break, TD | 159 MPa | 23000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 329 Polyester Film, 380 Gauge Melinex® 329 is an opaque white, non-pretreated, polyester film with good handling properties and a unique glossy appearance. It is used as a base for pressure sensitive labels, in security and ac.. |
|||
Film Tensile Strength at Break, TD | 159 MPa | 23000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 329 Polyester Film, 500 Gauge Melinex® 329 is an opaque white, non-pretreated, polyester film with good handling properties and a unique glossy appearance. It is used as a base for pressure sensitive labels, in security and ac.. |
|||
Film Tensile Strength at Break, TD | 159 MPa | 23000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 329 Polyester Film, 700 Gauge Melinex® 329 is an opaque white, non-pretreated, polyester film with good handling properties and a unique glossy appearance. It is used as a base for pressure sensitive labels, in security and ac.. |
|||
Film Tensile Strength at Break, TD | 159 MPa | 23000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 329 Polyester Film, 75 Gauge Melinex® 329 is an opaque white, non-pretreated, polyester film with good handling properties and a unique glossy appearance. It is used as a base for pressure sensitive labels, in security and ac.. |
|||
Film Tensile Strength at Break, TD | 159 MPa | 23000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 329 Polyester Film, 820 Gauge Melinex® 329 is an opaque white, non-pretreated, polyester film with good handling properties and a unique glossy appearance. It is used as a base for pressure sensitive labels, in security and ac.. |
|||
Film Tensile Strength at Break, TD | 159 MPa | 23000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 329 Polyester Film, 92 Gauge Melinex® 329 is an opaque white, non-pretreated, polyester film with good handling properties and a unique glossy appearance. It is used as a base for pressure sensitive labels, in security and ac.. |
|||
Film Tensile Strength at Break, TD | 159 MPa | 23000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 329S Polyester Film, 92 Gauge An opaque white film with good handling properties, a unique glossy appearance, and a lower shrinkage for special applicationsInformation provided by DuPont. |
|||
Film Tensile Strength at Break, TD | 159 MPa | 23000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 329W Polyester Film, 300 Gauge An opaque white film with good handling properties and a unique glossy appearance. 329W has same properties as 329 with the only exception being it is wound reverse. See the 329 datasheet for detail.. |
|||
Film Tensile Strength at Break, TD | 159 MPa | 23000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 339 Polyester Film, 1000 Gauge Melinex® 339 is an opaque white polyester film with good handling properties that is pre-treated on both surfaces to promote adhesion to most industrial coatings.Typical Applications: Melinex® 339.. |
|||
Film Tensile Strength at Break, TD | 159 MPa | 23000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 339 Polyester Film, 300 Gauge Melinex® 339 is an opaque white polyester film with good handling properties that is pre-treated on both surfaces to promote adhesion to most industrial coatings.Typical Applications: Melinex® 33.. |
|||
Film Tensile Strength at Break, TD | 159 MPa | 23000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 339 Polyester Film, 380 Gauge Melinex® 339 is an opaque white polyester film with good handling properties that is pre-treated on both surfaces to promote adhesion to most industrial coatings.Typical Applications: Melinex® 339.. |
|||
Film Tensile Strength at Break, TD | 159 MPa | 23000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 339 Polyester Film, 700 Gauge Melinex® 339 is an opaque white polyester film with good handling properties that is pre-treated on both surfaces to promote adhesion to most industrial coatings.Typical Applications: Melinex® 339.. |
|||
Film Tensile Strength at Break, TD | 159 MPa | 23000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 339 Polyester Film, 820 Gauge Melinex® 339 is an opaque white polyester film with good handling properties that is pre-treated on both surfaces to promote adhesion to most industrial coatings.Typical Applications: Melinex® 339.. |
|||
Film Tensile Strength at Break, TD | 159 MPa | 23000 psi | ASTM D882A |
DuPont Teijin Films Melinex® ST339 Polyester Film, 1000 Gauge Melinex® ST339 is a stabilized, opaque white polyester film with good handling and lay flat properties that is pre-treated on both surfaces to promote adhesion to most industrial coatings Typical A.. |
|||
Film Tensile Strength at Break, TD | 159 MPa | 23000 psi | ASTM D882A |
DuPont Teijin Films Melinex® ST339 Polyester Film, 200 Gauge Melinex® ST339 is a stabilized, opaque white polyester film with good handling and lay flat properties that is pre-treated on both surfaces to promote adhesion to most industrial coatings Typical A.. |
|||
Film Tensile Strength at Break, TD | 159 MPa | 23000 psi | ASTM D882A |
DuPont Teijin Films Melinex® ST339 Polyester Film, 300 Gauge Melinex® ST339 is a stabilized, opaque white polyester film with good handling and lay flat properties that is pre-treated on both surfaces to promote adhesion to most industrial coatings Typical A.. |
|||
Film Tensile Strength at Break, TD | 159 MPa | 23000 psi | ASTM D882A |
DuPont Teijin Films Melinex® ST339 Polyester Film, 380 Gauge Melinex® ST339 is a stabilized, opaque white polyester film with good handling and lay flat properties that is pre-treated on both surfaces to promote adhesion to most industrial coatings Typical A.. |
|||
Film Tensile Strength at Break, TD | 159 MPa | 23000 psi | ASTM D882A |
DuPont Teijin Films Melinex® ST339 Polyester Film, 500 Gauge Melinex® ST339 is a stabilized, opaque white polyester film with good handling and lay flat properties that is pre-treated on both surfaces to promote adhesion to most industrial coatings Typical A.. |
|||
Film Tensile Strength at Break, TD | 159 MPa | 23000 psi | ASTM D882A |
DuPont Teijin Films Melinex® ST339 Polyester Film, 700 Gauge Melinex® ST339 is a stabilized, opaque white polyester film with good handling and lay flat properties that is pre-treated on both surfaces to promote adhesion to most industrial coatings Typical A.. |
|||
Film Tensile Strength at Break, TD | 159 MPa | 23000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 339 Polyester Film, 500 Gauge Melinex® 339 is an opaque white polyester film with good handling properties that is pre-treated on both surfaces to promote adhesion to most industrial coatings.Typical Applications: Melinex® 339.. |
|||
Film Tensile Strength at Break, TD | 159 MPa | 23000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 487 Polyester Film, 200 Gauge Melinex® 487 is a high-yield, white film that is coated on one side for adhesion to inks, coatings, laser printing, and thermal transfer printing.Information provided by DuPont. |
|||
Film Tensile Strength at Break, TD | 159 MPa | 23000 psi | ASTM D882A |
DuPont Teijin Films Mylar® MLB Polyester Film, 300 Gauge Product Description: Mylar® MLB is an uncoated, transparent, polyester film designed for use as a component of a lamination structure and may be suitable for use in medical applications. Mylar® ML.. |
|||
Film Tensile Strength at Break, TD | 159 MPa | 23000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 339 Polyester Film, 200 Gauge Melinex® 339 is an opaque white polyester film with good handling properties that is pre-treated on both surfaces to promote adhesion to most industrial coatings.Typical Applications: Melinex® 339.. |