Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 14.0 MPa | 2030 psi | ASTM D882 |
Petroquimica Triunfo Trithene® CX 7065 LDPE - Extrusion Coating The Trithene® CX 7065 resin is a product developed especially to meet the segment of extrusion coating where the following properties are necessary: processing stability at high production rates, a.. |
|||
Film Tensile Strength at Break, TD | 14.0 MPa | 2030 psi | ASTM D882 |
Westlake EMAC® SP2242 Specialty Copolymer
(discontinued **) EMAC resins adhere to and are compatible with a wide range of materials including paper, polyolefins, oriented polyolefins, polyesters, ionomers, PVdC, unplasticized PVC and other polar polymers. Fo.. |
|||
Film Tensile Strength at Break, TD | 14.0 MPa | 2030 psi | ASTM D882 |
Huntsman PE1058 Film Extrusion Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Exceptional draw down and processability, excellent strength, good heat sealability, and optics.Applications: Film extrusion: all thin film uses and especiall.. |
|||
Film Tensile Strength at Break, TD | 14.0 MPa | 2030 psi | ASTM D882 |
Huntsman PE1068 Film Extrusion Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Exceptional draw down and processability even to 1/2 mil; excellent strength, good heat sealability, and good optical.FDA Notes: Conforms to FDA regulation 21.. |
|||
Film Tensile Strength at Break, TD | 14.0 MPa | 2030 psi | ASTM D882 |
Huntsman PE5030 Extrusion Coating Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Good draw down, low neck-in, good heat sealability and adhesion, low smoking, and excellent printabilityApplications: Extrusion: coating grade and general coa.. |
|||
Film Tensile Strength at Break, TD | 14.0 MPa | 2030 psi | ASTM D882 |
Huntsman PE5032 Extrusion Coating Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Excellent draw down, low neck-in, excellent heat sealability, good adhesion, low smoking, no edge weave, and excellent printability.Applications: Extrusion: c.. |
|||
Film Tensile Strength at Break, TD | 14.0 MPa | 2030 psi | ASTM D822 |
Westlake EMAC® Plus SP1358 21.5% Ethylene-Methyl Acrylate Copolymer Westlake EMAC® Plus SP1358 is a 21.5% EMA copolymer containing slip and antiblock. This resin is designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low.. |
|||
Film Tensile Strength at Break, TD | 14.0 MPa | 2030 psi | ASTM D882 |
Huntsman Rexell® V3401 Blown Film Extrusion LLDPE
(discontinued **) Ultra linear low density copolymer, cast film extrusion, FDA compliant.Features: Excellent processability, toughness, and optics with good sealing properties.Applications: Sealing layer in coextrude.. |