Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 12.4 MPa | 1800 psi | ASTM D882 |
Dow DAF 780 Carpet Underlayment Adhesion Film DAF 780 is a low melt point, coextruded film used to improve slip characteristics of polyurethane foam for carpet installation or other applications.Information provided by Dow |