Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 100 MPa | 14500 psi | ASTM D882 |
Honeywell Aegisâ„¢ H135MP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H135MP is a lubricated and nucleated high viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR.. |
|||
Film Tensile Strength at Break, TD | 100 MPa | 14500 psi | ASTM Data |
Styrolution Styrolux 684D SBC Styrolux 684D is a thermoplastic styrene-butadiene block copolymer which is suitable for injection molding, extrusion, and thermoforming. It offers an outstanding combination of crystal clarity and.. |
|||
Film Tensile Strength at Break, TD | 100 MPa | 14500 psi | ISO 527-3 |
EMS-Grivory Grivory® HB 5299 HV PA* Product description: Grivory HB 5299 HV is a lubricated, lactam free copolyamide, especially developed for high barrier (oxygen, carbon dioxide) packaging solutions. HV indicates high viscosity, sui.. |
|||
Film Tensile Strength at Break, TD | 100 MPa | 14500 psi | ISO 527-3 |
EMS-Grivory Grivory® HB5299 PA* Product description: Grivory HB 5299 is a lubricated, lactam free copolyamide, especially developed for high barrier (oxygen, carbon dioxide) packaging solutions. Excellent oxygen and carbon dioxide.. |