Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | >= 1000 g | >= 2.20 lb | ASTM D1709/A |
NOVA Chemicals Sclair® FP112-A Octene VLDPE Film Resin Features: Low seal initiation temperatureHigh toughnessVery good optical propertiesComplies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Low gel Applications: Sealant and lamination film for food packagi.. |
|||
Dart Drop Test | >= 1000 g | >= 2.20 lb | F50; ASTM D1709 |
ExxonMobil Exceed™ 350D65 LDPE/Hexene Tough Premium Liner Film Resin, 0.8 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer produced using Exxon Chemical's EXXPOL® technology. Films made from EXCEED 350D65 resin have outstanding tensile, impact streng.. |
|||
Dart Drop Test | >= 1000 g | >= 2.20 lb | 50µ; ISO 7765-1 |
Total Evatane® 24 - 03 HDPE vinyl acetate copolymer, blown film, injection molding
(discontinued **) EVA Copolymer made by high pressure tubular process. Temperature profile (°C) for injection molding: 130 to 160.Information provided provided by Total Petrochemicals.Total Petrochemicals includes f.. |
|||
Dart Drop Test | >= 1000 g | >= 2.20 lb | 50µ; ISO 7765-1 |
Total Evatane® 28 - 03 HDPE, blown film
(discontinued **) EVA Copolymer made by high pressure tubular process. Temperature profile (°C) for injection molding: 130 to 160.Information provided provided by Total Petrochemicals.Total Petrochemicals includes f.. |
|||
Dart Drop Test | >= 1000 g | >= 2.20 lb | 50µ; ISO 7765-1 |
Total Evatane® 28 - 05 HDPE vinyl acetate copolymer, blown film, injection molding
(discontinued **) EVA Copolymer made by high pressure tubular process. Temperature profile (°C) for injection molding: 120 to 150.Information provided provided by Total Petrochemicals.Total Petrochemicals includes f.. |
|||
Dart Drop Test | >= 1000 g | >= 2.20 lb | Using 2 in. (0.508 cm) dia dart, 60 in. (774 cm) drop height. |
Kraton® D1102 + LDPE blend (50/50) Blending KRATON D and G polymers with PE significantly improves the toughness at both room and low temperatures. KRATON polymers are block segments of styrene and rubber monomers (A-B, A-B-A, or [A.. |
|||
Dart Drop Test | >= 1000 g | >= 2.20 lb | Method B; ASTM D1709 |
Styrolution Styroflex® 2G 66 SBC Description: Styroflex® 2G 66 is a styrene-butadiene block copolymer (SBC) with the properties of a thermoplastic elastomer (S-TPE). Styroflex® 2G 66 is the only S-TPE with a styrene content o.. |
|||
Dart Drop Test | >= 1000 g | >= 2.20 lb | ASTM D1709 |
M. Holland Company MAGMA® LM311-DX LLDPE
(discontinued **) Features: Good Processability, Good Puncture Resistance, Good Tear Strength, Good ToughnessProcessing Method: ExtrusionInformation provided by M. Holland. |
|||
Dart Drop Test | >= 1000 g | >= 2.20 lb | ASTM D1709 |
M. Holland Company MAGMA® LM311-D LLDPE
(discontinued **) Features: Good Processability, Good Puncture Resistance, Good Tear Strength, Good ToughnessProcessing Method: ExtrusionInformation provided by M. Holland. |