Polymer Property : Dart Drop Test = 1.17 lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop Test 530 g
1.17 lb
ASTM D1709
M. Holland Company MAGMA® LL1091 LLDPE  (discontinued **)
Features: Good Heat Seal, Good ToughnessUses: PackagingProcessing Method: ExtrusionInformation provided by M. Holland.
Dart Drop Test 530 g
1.17 lb
Method B; ASTM D1709
Dow ELITE™ 5500G Enhanced Polyethylene Resin
™ 5500G is a copolymer produced via INSITE™ Technology. It offers an exceptional combination of processability, low heat seal initiation temperature, package integrity, optical properties, and te..