Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Dart Drop Test = 0.904 lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop Test 410 g
0.904 lb
F50; ASTM D-1709
ExxonMobil Escorene® LD-768 High EVA Film and Compounding Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A low gel 27.5% vinyl acetate copolymer designed for film and compounding applications. The resin provides very low modulus films with high tensile..
Dart Drop Test 410 g
0.904 lb
ASTM-D1709 (Method B)
Braskem TU3001 LDPE Blown Film Extrusion Polyethylene
TU3001 is a low-density polyethylene (LDPE) with high molecular weight, excellent mechanical properties, and good processability. These qualities ensure the production of films with uniform thicknes..
Copyright © lookpolymers.com All Rights Reserved