Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 400 g | 0.882 lb | F50; ISO 7765-1 |
Polimeri Europa Greenflex® FL 25 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion Greenflex FL 25 is an ethylene vinyl acetate copolymer (EVA) for blown film extrusion. Films produced with Greenflex FL 25 show good optical properties and excellent sealability.Main Applications: .. |
|||
Dart Drop Test | 400 g | 0.882 lb | F50; ASTM D 1709/A |
NOVA Chemicals Surpass® FPs117-C Octene Copolymer sLLDPE Film Resins FPs117-C complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food, without .. |
|||
Dart Drop Test | 400 g | 0.882 lb | Modified 12.7 mm (0.5 in.) dia. head, 127 mm (5 in.) dia. clamp, 660 mm (26 in.) drop. Value at -18°C (0°F) is 500 g.; ASTM D1709A |
Eastman EASTALLOY Polymer DA003-8999K, Clear Alloy
(discontinued **) Properties below based on a film thickness of 250 microns. CO2 Permeability is 49 cm3·mm/m2·24h·atm per ASTM D 1434.Product Description: EASTALLOY DA003-8999K Polymer is a clear copolyester/pol.. |
|||
Dart Drop Test | 400 g | 0.882 lb | ASTM D1709 |
Huntsman Rexell® V8801 Cast Film Extrusion LLDPE
(discontinued **) Linear-low very low density copolymer, blown film extrusion, FDA compliantFeatures: Excellent resistance to impact, puncturing, tearing, and flex cracking with good weld seal strength, hot tack, and.. |
|||
Dart Drop Test | 400 g | 0.882 lb | Impact Strength, ASTM D1709-62T |
DuPont™ Dartek® N-201 Nylon 6,6 Non-Forming Film, 25 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.A nylon film made from type 6,6 polymer - the condensation product of adipic acid and hexamethylene diamine. Primarily formulated for pouch and primal bag .. |
|||
Dart Drop Test | 400 - 600 g | 0.882 - 1.32 lb | Average value: 550 g Grade Count:4 |
Overview of materials for Nylon 66, Film This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Film". Each property range of values reported is minimum and maximum values of appropriate Mat.. |
|||
Dart Drop Test | >= 400 g | >= 0.882 lb | ASTM D1709 |
LG Chemical SEETEC EF321 Ethylene Vinyl Acetate Characteristics: Good Mechanical Properties. Good Optical Properties. Additives : No Additive Applications: Agricultural FilmCSA No. 25895-47-0Information provided by LG Chemical |
|||
Dart Drop Test | >= 400 g | >= 0.882 lb | ASTM D1709 |
LG Chemical SEETEC EF443 Ethylene Vinyl Acetate Characteristics: Good Mechanical Properties and Good Optical PropertiesApplications: Agricultural FilmCSA No. 24937-78-8Information provided by LG Chemical |
|||
Dart Drop Test | >= 400 g | >= 0.882 lb | ASTM D1709 |
LG Chemical SEETEC ES440 Ethylene Vinyl Acetate Characteristics: Good Mechanical Properties and Good Optical PropertiesApplications: Agricultural Film, Shoe solesCSA No. 24937-78-8Information provided by LG Chemical |
|||
Dart Drop Test | 400 g | 0.882 lb | ASTM D1709 |
LG Chemical SEETEC ST308 Linear Low Density Polyethylene, Blown Film Grade Features: Characteristics- Excellent puncture resistance, tear strength. Excellent sealing and optical properties. Comonomer: Octene-1. Additives- Medium slip agent, Medium antiblocking agentApplica.. |
|||
Dart Drop Test | 400 g | 0.882 lb | ASTM D1709 |
Solvay Specialty Polymers Ajedium™ Film Thermoplastic Polyimide (PI, TP) TPI is a thermoplastic polyimide film that has excellent, thermal, chemical, electrical and physical properties. With a continuous use temperature to 240°C (465°F), TPI films offer superior ra.. |
|||
Dart Drop Test | 400 g | 0.882 lb | ASTM D1709 |
Solvay Specialty Polymers Ajedium™ Films -- Udel® PSU P-1700 NT-11 Polysulfone (PSU) Udel® P-1700 polysulfones are tough, high-strength thermoplastics that are suitable for continuous use up to 300°F (149°C). Udel Film is resistant to oxidation and hydrolysis and withstand .. |
|||
Dart Drop Test | 400 g | 0.882 lb | ISO 7765-1 |
Total EVA 1020 VN 3 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1020 VN 3 is made by a high pressure tubular process. Grade for flexible, very transparent films with high strength and very good sealability. Contains an antioxidant.Application examples: Thi.. |
|||
Dart Drop Test | 400 g | 0.882 lb | Method A; ASTM D1709 |
Dow DOWLEX™ 2085G Polyethylene Resin DOWLEX™ 2085G is an ethylene-octene copolymer designed for general purpose thin gauge film applications. It is perfect for high strength consumer trash bags/liners. This product can be used in ot.. |
|||
Dart Drop Test | 400 g | 0.882 lb | |
Dow Elite® 5110 Linear Low Density Polyethylene 5110 enhanced polyethylene resin is a copolymer produced via INSITE Technology from Dow Plastics. It offers unique combination of high modulus and excellent impact strength, allowing for downgaugin.. |
|||
Dart Drop Test | 400 g | 0.882 lb | ASTM D1709 |
Arkema Group OREVAC® 9304 EVA Terpolymer OREVAC® is a range of ethylene-vinyl acetate copolymers modified by adjunction of polar groups which, when molten, have excellent adhesive properties to various substrates. They are supplied as fre.. |
|||
Dart Drop Test | 400 g | 0.882 lb | 50 microns film |
Arkema Group Orevac® 9304 Film EVA-MAH Terpolymer EVA Terpolymers based Main Applications: Extrusion coating Thermo-adhesive filmsInformation provided by Arkema Group |
|||
Dart Drop Test | 400 g | 0.882 lb | F<sub>50</sub>; ASTM D-1709 |
Bapolene® 142A Polyethylene Film Grade Bapolene 142A is a hexene linear low density polyethylene for blown film applications requiring superior impact strength. Product is designed to exhibit performance similar to that of super hexene p.. |
|||
Dart Drop Test | 400 g | 0.882 lb | F<sub>50</sub>; ASTM D-1709 |
Bapolene® 142B Polyethylene Film Grade Bapolene 142B is a hexene linear low density polyethylene for blown film applications requiring superior impact strength. Product is designed to exhibit performance similar to that of super hexene p.. |
|||
Dart Drop Test | 400 g | 0.882 lb | F<sub>50</sub>; ASTM D-1709 |
Bapolene® 142F Polyethylene Film Grade Bapolene 142F is a hexene linear low density polyethylene for blown film applications requiring superior impact strength. Product is designed to exhibit performance similar to that of super hexene p.. |
|||
Dart Drop Test | 400 g | 0.882 lb | ASTM D1709 |
Huntsman Rexell® V8403 Cast Film Extrusion LLDPE
(discontinued **) Linear-low very low density copolymer, blown film extrusion, FDA compliantFeatures: Excellent resistance to impact, puncturing, tearing, and flex cracking with good weld seal strength, hot tack, and.. |
|||
Dart Drop Test | 400 g | 0.882 lb | F50; ISO 7765-1 |
Polimeri Europa Clearflex® H&T LGH 108 Octene Copolymer Linear Low Density Polyethylene Clearflex H&T LGH 108 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidants and processing aid, suitable for blown film extrusion.Films obtained from Clearflex H&T LGH.. |
|||
Dart Drop Test | 400 g | 0.882 lb | F-50 at 26 in.; ASTM D1709 |
Chevron Phillips Vytek™ V208A3 Enhanced LLDPE Blown Film Resin
(discontinued **) Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: excellent dart impact, hot-tack and heat seal properties, good drawdown, can be use.. |