Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 5.90 g | 0.0130 lb | |
DuPont Nucrel® 903 Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film 9 wt% Methacrylic Acid.Nucrel® 0903 is an ethylene-methacrylic acid copolymer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process pol.. |
|||
Dart Drop Test | 5.90 - 370 g | 0.0130 - 0.816 lb | Average value: 141 g Grade Count:4 |
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene-Methyl Acrylate Copolymer, Film Grade". Each property range of values reported is minimum and m.. |