Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 410 g | 0.904 lb | F50; ASTM D-1709 |
ExxonMobil Escorene® LD-768 High EVA Film and Compounding Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A low gel 27.5% vinyl acetate copolymer designed for film and compounding applications. The resin provides very low modulus films with high tensile.. |
|||
Dart Drop Test | 410 g | 0.904 lb | ASTM-D1709 (Method B) |
Braskem TU3001 LDPE Blown Film Extrusion Polyethylene TU3001 is a low-density polyethylene (LDPE) with high molecular weight, excellent mechanical properties, and good processability. These qualities ensure the production of films with uniform thicknes.. |