Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 40.0 g | 0.0882 lb | F50; ISO 7765-1 |
Polimeri Europa Clearflex® CL 508 Octene Copolymer Linear Medium Density Polyethylene Clearflex CL 508 is an octene copolymer linear medium density polyethylene (C8-LMDPE), with antioxidants, suitable for cast film extrusion.Films manufactured with Clearflex CL 508 exhibit a good bal.. |
|||
Dart Drop Test | 40.0 g | 0.0882 lb | 1.1; ASTM D 1709/A |
NOVA Chemicals Sclair® 17A Butene HDPE Film Resin 17A complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food, without te.. |
|||
Dart Drop Test | 40.0 g | 0.0882 lb | F50; ASTM D 1709/A |
NOVA Chemicals Surpass® FPs236-A Octene sMDPE Film Resin FPs236-A complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food. FPs236-.. |
|||
Dart Drop Test | <= 40.0 g | <= 0.0882 lb | F50; ASTM D1709 |
ExxonMobil Escorene® LD-102 LDPE Drawdown Resin, 0.5 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer, good clarity, laundry and dry cleaning film resin capable of providing a tough film in very thin gauges.Applications: Dry cleaning es.. |
|||
Dart Drop Test | 40.0 g | 0.0882 lb | ASTM D1709/A |
NOVA Chemicals Sclair® 94E Butene LMDPE Film and Extrusion Resin Features: Excellent processabilityGood stiffness and strengthHigh stretchability Applications: Overwrap filmNettingBlend resinInformation provided by Nova Chemicals |
|||
Dart Drop Test | 40.0 g | 0.0882 lb | ASTM D1709 |
LyondellBasell Petrothene® LP510300 High Density Polyethylene ApplicationsPETROTHENE LLP 5103-00 is a copolymer resin designed for blown film applications. This resin offers high stiffness, excellent appearance and bubble stability and good drawdown. It is r.. |
|||
Dart Drop Test | 40.0 g | 0.0882 lb | F<sub>50</sub>; ASTM D1709 |
LyondellBasell Petrothene® LP540200 High Density Polyethylene ApplicationsPETROTHENE LP 5402-00 is a copolymer resin designed for blown film applications. This resin offers high stiffness, excellent appearance and bubble stability and good draw-down. LP 5402-0.. |
|||
Dart Drop Test | 40.0 g | 0.0882 lb | ISO 7765-1 |
Total Lumicene® mPE M6040 S01 Metallocene Polyethylene, Cast Film Lumicene® mPE M 6040 S01 is a second generation metallocene high density polyethylene.Lumicene® mPE M 6040 S01 can be processed at high output rates with low extrusion pressure, low neck-in, excel.. |
|||
Dart Drop Test | <= 40.0 g | <= 0.0882 lb | ASTM D1709A |
ExxonMobil HDPE HD 7845.30 High Density Polyethylene Resin Product Description: HD 7845.30 can be processed on high stalk, pocket extrusion or cast lines. Films made from HD 7845.30 exhibit an excellent stiffness balance. High thermal stability provides exc.. |
|||
Dart Drop Test | 40.0 g | 0.0882 lb | ASTM D1709 |
Huntsman Rexell® M3109 Blown Film Extrusion LLDPE
(discontinued **) Linear-low medium density copolymer and FDA compliant.Features: Excellent combination of stiffness, heat resistance, and impermeability to water vapor.Applications: Food packaging, multi-layer syste.. |
|||
Dart Drop Test | 40.0 - 100 g | 0.0882 - 0.221 lb | Average value: 71.1 g Grade Count:9 |
Overview of materials for Linear Medium Density Polyethylene (LMDPE), Film This property data is a summary of similar materials in the MatWeb database for the category "Linear Medium Density Polyethylene (LMDPE), Film". Each property range of values reported is minimum and.. |
|||
Dart Drop Test | 40.0 - 1500 g | 0.0882 - 3.31 lb | Average value: 178 g Grade Count:217 |
Overview of materials for Low Density Polyethylene (LDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Film Grade". Each property range of values reported is minimum and maxi.. |