Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 373 g | 0.822 lb | ASTM D1709 |
Formosa Plastics Formolene® E927ND Film HDPE High Molecular Weight High Density Polyethylene (HMW-HDPE) for Film Extrusion Formolene® E927ND is a bi-modal HMW-HDPE resin designed for high dart impact strength and good processing characteristi.. |