Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 325 - 1000 g | 0.717 - 2.20 lb | Average value: 519 g Grade Count:5 |
Overview of materials for Styrene-Butadiene Copolymer, SBC This property data is a summary of similar materials in the MatWeb database for the category "Styrene-Butadiene Copolymer, SBC". Each property range of values reported is minimum and maximum values .. |
|||
Dart Drop Test | 325 g | 0.717 lb | 26 in; ASTM D1709 |
Chevron Phillips K-Resin® DK13 Styrene-Butadiene Copolymer, Film Grade
(discontinued **) Styrene-Butadiene Copolymer. Properties below based on 1 mil ( 0.025 mm) film; 2.5:1 Blow Up Ratio; 35 mil (0.90 mm) die gap.Customer Benefits: DK13 is an SBC designed for the film market and has i.. |