Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 220 g | 0.485 lb | F<sub>50</sub>; ASTM D1709 |
LyondellBasell Petrothene® NA942094 Low Density Polyethylene ApplicationsPETROTHENE NA 942 is a series of resins designed especially for heavy duty film applications, such as bags used to package fertilizer, peat moss, decorative stone, and agricultural and c.. |
|||
Dart Drop Test | 220 g | 0.485 lb | ASTM D1709 |
LG Chemical LUTENE BB0808 LDPE Blown Film Grade Description: LUTENE BB0808 is mainly intended for the extrusion of blown film with high mechanical property for the manufacture of shrink film and pallet shrink covers. LUTENE BB0808 have the balanc.. |
|||
Dart Drop Test | 220 g | 0.485 lb | ASTM D1709-98 |
Ipiranga Petrochem LB 0120 BS LLDP IPQ produces Linear Low Density Polyethylene (LLDPE) for use by plastics molding industry segments that employ extrusion processes in the manufacturing of films destined for producing bobbins and ba.. |
|||
Dart Drop Test | 220 g | 0.485 lb | ASTM D1709 |
Iran Petrochemical (PCC) EX 4 HM9455 F High Density Polyethylene EX4 is a high density polyethylene with 1-Butene as co monomer. It is high rigidity, low gel level, high drowdown, somewhat stiffer than EX 5.Applications: film extrusion, blending partner, refuse .. |
|||
Dart Drop Test | 220 g | 0.485 lb | ASTM D1709 |
Iran Petrochemical (PCC) EX 5 HM 9450 F High Density Polyethylene EX5 is a high density polyethylene with 1-Butene as co monomer.Applications: film extrusion, counter bag, carrier bag, wrapping filmsInformation provided by Iran Petrochemical Commercial Co. |
|||
Dart Drop Test | 220 g | 0.485 lb | F<sub>50</sub>; ASTM D1709 |
LyondellBasell Petrothene® NA940085 Low Density Polyethylene (Film Grade) ApplicationsPETROTHENE NA 940 is a series of resins designed for heavy duty film applications. Superior puncture resistance combined with excellent impact properties make NA 940 an ideal choice for.. |
|||
Dart Drop Test | 220 g | 0.485 lb | F<sub>50</sub>; ASTM D1709 |
LyondellBasell Petrothene® NA940094 Low Density Polyethylene (Film Grade) ApplicationsPETROTHENE NA 940 is a series of resins designed for heavy duty film applications. Superior puncture resistance combined with excellent impact properties make NA 940 an ideal choice for.. |
|||
Dart Drop Test | 220 g @Thickness 0.0250 mm |
0.485 lb @Thickness 0.000984 in |
ISO 7765-1 |
Borealis Borstar® FB1350 Medium Density Polyethylene Borstar® FB1350 is a linear medium density polyethylene grade combining excellent extrusion properties with high film stiffness. Borstar® FB1350 is well suited for mono- and coextrusion of films .. |
|||
Dart Drop Test | 220 g | 0.485 lb | ISO 7765-1 |
Total Lumicene® mPE M 2704 EP S01 Metallocene Polyethylene, Blown Film This product is a Total Ecosolutions grade.Lumicene® mPE M 2704 EP S01 is a second generation metallocene based Low Density Polyethylene with hexene as comonomer.Lumicene® mPE M 2704 EP S01 can be.. |
|||
Dart Drop Test | 220 g | 0.485 lb | ASTM D1709A |
ExxonMobil Optema® TC-110 Cast Ethylene Methyl Acrylate Product Description: Optema TC 110 is an ethylene methyl acrylate copolymer specifically formulated to offer extrusion and property performance for blown and cast film applications. It can produce f.. |
|||
Dart Drop Test | 220 g | 0.485 lb | F<sub>50</sub>; ASTM D1709 |
LyondellBasell Petrothene® NA940000 Low Density Polyethylene (Film Grade) ApplicationsPETROTHENE NA 940 is a series of resins designed for heavy duty film applications. Superior puncture resistance combined with excellent impact properties make NA 940 an ideal choice for.. |