Mechanical Properties Metric English Comments
Dart Drop Test 135 g
0.298 lb
ASTM D1709
SABIC 518N Linear Low Density Polyethylene for Blown Film
Product Description: 548N is a fractional melt index Linear Low Density Polyethylene grade suitable for high strength packaging applications. Films produced using this resin yield outstanding toug..
Dart Drop Test 135 g
0.298 lb
(method A); ASTM D1709
Petroquimica Triunfo Trithene® TS 7028 LDPE - Automatic Packaging
The Trithene TS 7028 resin is a low-density polyethylene (LDPE) with excellent optical and processability properties that allows for the production of films combining appearance, mechanical strength..
Dart Drop Test 135 g
0.298 lb
ASTM D1709
Formosa Plastics Formolene® L42009F Film (Butene Grade) LLDPE
Extra High Molecular Weight Hexene Copolymer Formolene® L42009F is a general-purpose film grade linear low density made using gas-phase technology. The resin exhibits excellent toughness and streng..
Dart Drop Test 135 g
0.298 lb
ASTM D1709
Formosa Plastics Formolene® L42009PE Film (Butene Grade) LLDPE
Linear Low Density Polyethylene Butene Copolymer for Film Extrusion Formolene® L42009PE is a general-purpose film grade linear low density made using gas-phase technology. The resin exhibits excell..
Dart Drop Test 135 g
0.298 lb
F50; ASTM D-1709
ExxonMobil Escorene® LD-331 EVA Film Resin, Very High Clarity, Very High Impact  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 5.8% vinyl acetate copolymer, high clarity film resin. Film made from this resin exhibits superior impact strength and heat sealability.Applicati..