Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Test | 134 g | 0.295 lb | Method A; ASTM D1709 |
Dow DOWLEX™ 2045.11G Linear Low Density Polyethylene For high speed, thin film applications Additional thermal stability Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow |
|||
Dart Drop Test | 134 g | 0.295 lb | Method A; ASTM D1709 |
Dow TUFLIN™ HSE-7002 NT 7 Linear Low Density Polyethylene Resin Industrial pallet wrap stretch film applications Premium film packaging applications Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a TUFLIN™ HSE-7002 NT 7 is an ethylene-hexene-1 copolymer, design.. |
|||
Dart Drop Test | 134 g | 0.295 lb | ASTM D1709 |
Huntsman Rexell® L8404 Cast Film Extrusion LLDPE
(discontinued **) Linear-low density copolymer, and FDA compliant.Applications: Blown film extrusion: general purpose.Film properties based on 1.0 guage (25 µm) thickness; blow-up ratio 2:1.Information provided by H.. |