Polymer Property : Elmendorf Tear Strength, TD = 81.3 g/mil Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 3.20 g/micron
81.3 g/mil
ASTM D1922
NOVA Chemicals Novapol® LF-Y320-C Fractional Melt LDPE Film Resin
Features: High melt strength and superior bubble stabilityEnhances throughputs in LLDPE blendsSuperior strength and toughnessExcellent shrink film characteristics Applications: Industrial packagingL..
Elmendorf Tear Strength, TD 3.20 g/micron
81.3 g/mil
ASTM D1922
NOVA Chemicals Novapol® LF-Y320-D Fractional Melt LDPE Film Resin
Features: High melt strength and superior bubble stabilityEnhances throughputs in LLDPE blendsSuperior strength and toughnessExcellent shrink film characteristics Applications: Industrial packagingL..