Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 30.7 g/micron
780 g/mil
ASTM D1922
Chevron Phillips Vytek™ V208C3 Enhanced LLDPE Blown Film Resin  (discontinued **)
Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: excellent dart impact, hot-tack and heat seal properties, good drawdown, can be use..
Elmendorf Tear Strength, TD 30.7 g/micron
780 g/mil
ASTM D1922
ExxonMobil LL 3201.36 Premium High Strength Film Resin
Product Description: LL 3201 resins are LLDPE hexane copolymer film resins. Films made from LL 3201 resins have outstanding tensile, stiffness and toughness properties. These superior properties, al..
Elmendorf Tear Strength, TD 30.7 g/micron
780 g/mil
ASTM D1922
ExxonMobil LL 3201.69 Premium High Strength Film Resin
Product Description: LL 3201 resins are LLDPE hexane copolymer film resins. Films made from LL 3201 resins have outstanding tensile, stiffness and toughness properties. These superior properties, al..
Elmendorf Tear Strength, TD 30.7 g/micron
780 g/mil
ASTM D1922
ExxonMobil HD 7845.30 MMW Blown Film Resin
Product Description: HD 7845.30 can be processed on high stalk, pocket extrusion or cast lines. Films made from HD 7845.30 exhibit an excellent stiffness balance. High thermal stability provides exc..