Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 0.300 g/micron | 7.62 g/mil | |
DuPont™ Surlyn® 1605 Sodium Ionomer Resin for Blown/Cast Film and Extrusion Coating Surlyn® 1605 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment and extrusion coating and coextrusion coating equipment designed to proces.. |
|||
Elmendorf Tear Strength, TD | 0.300 - 11.0 g/micron | 7.62 - 279 g/mil | Average value: 2.27 g/micron Grade Count:17 |
Overview of materials for Ionomer, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Ionomer, Film Grade". Each property range of values reported is minimum and maximum values of appropriat.. |