Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 26.67 g/micron | 677.4 g/mil | ASTM D1922 |
SABIC 6318B Linear Low Density Polyethylene for Cast Film Product Description: 6318B is a hexene copolymer Linear Low Density Polyethylene grade designed to provide easy processability and specially formulated for optimum thermal stability at high process.. |